System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Shandong Dawn Dawnprene 13-55A TPV (EPDM/PP)
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Thermoplastic Vulcanizate Elastomer (TPV)
Material Notes:
Uses: Automotive - Glass Run Channel: Lips, lip soft part for inner beltline, windshield strip/sun trim strip, sunroof trim strip.
Information provided by Shandong Dawn Polymer Material Co.,Ltd.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.935
g/cc
0.0338
lb/in³
ISO 1183
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
58
58
ISO 7619
50
@Treatment Temp. 80.0 °C,
Time 86400 sec
50
@Treatment Temp. 176 °F,
Time 24.0 hour
After Heat Aging; ISO 188
Tensile Strength
5.50
MPa
798
psi
ISO 37
Elongation at Break
400 %
400 %
ISO 37
Compression Set
28 %
@Temperature 70.0 °C,
Time 79200 sec
28 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
Descriptive Properties
Accelerated Weathering SAE J2527
0.7
Delta E, 2500KJ
Elongation Change (%) ISO 188
-15.5
change @ heat aging 100°C, 1000hr
Tensile Change (%) ISO 188
-8.4
change @ heat aging 100°C, 1000hr
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer
Shandong Dawn Dawnprene 13-67A TPV (EPDM/PP)
Shandong Dawn Dawnprene 13-65A TPV (EPDM/PP)
Shandong Dawn Dawnprene 13-73AW TPV (EPDM/PP)
Shandong Dawn Dawnprene 14-65A TPV (EPDM/PP)
PSHAND901 / 192541
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.