MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® Redux® 312 Modified epoxy film adhesive (0.015 psf)
Categories: Polymer; Adhesive; Film; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A supported version, Redux® 312/5, is available with a woven nylon carrier for bond line thickness control.

Features: Short cure cycle - cures in 30 minutes at 250°F; Good mechanical performance up to 210°F; Suitable for composite to composite bonding; Low volatile content (solventless process).
Applications: Metal to metal bonding; Sandwich constructions; Composite to composite bonding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 4.60 ksi
@Temperature 79.4 °C
Lap Shear
 4.80 ksi
@Temperature 71.1 °C
Lap Shear
 5.40 ksi
@Temperature 21.1 °C
Lap Shear
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature -17.8 °C
 
Descriptive Properties
Areal Weight (psf)0.015
Roll Width (in)21
Standard Roll (ft2)645

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 9392 Flexible Potting Epoxy Adhesive
Overview of materials for Epoxy Adhesive
Hexcel® Redux® 312 Modified epoxy film adhesive (0.06 psf)
Henkel Hysol EA 9321 Paste Adhesive System

PHEXC434 / 99253

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.