MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® Redux® 312 Modified epoxy film adhesive (0.06 psf)
Categories: Polymer; Adhesive; Film; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A supported version, Redux® 312/5, is available with a woven nylon carrier for bond line thickness control.

Features: Short cure cycle - cures in 30 minutes at 250°F; Good mechanical performance up to 210°F; Suitable for composite to composite bonding; Low volatile content (solventless process).
Applications: Metal to metal bonding; Sandwich constructions; Composite to composite bonding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 9.10 MPa
@Temperature 21.1 °C
1320 psi
@Temperature 70.0 °F
Flatwise Tensile
Shear Strength  29.6 MPa
@Temperature 98.9 °C
4300 psi
@Temperature 210 °F
Lap Shear
 39.3 MPa
@Temperature 71.1 °C
5700 psi
@Temperature 160 °F
Lap Shear
 42.7 MPa
@Temperature 21.1 °C
6200 psi
@Temperature 70.0 °F
Lap Shear
Peel Strength 9.12 kN/m
@Temperature 21.1 °C
52.0 pli
@Temperature 70.0 °F
Bell Peel
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature -17.8 °C
12.0 Month
@Temperature 0.000 °F
 
Descriptive Properties
Areal Weight (psf)0.06
Climbing Drum Peel (in-lb/3in)8070°F
Roll Width (in)21
Standard Roll (ft2)645

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® Redux® 312/5 Modified epoxy film adhesive
Hexcel® Redux® 312 Modified epoxy film adhesive (0.015 psf)
Solvay FM® 377U psf 0.055 (269 gsm) Adhesive Film
Phosphorus (V) Sulfide Trifluoride, PSF3
Hexcel® Redux® 340U(SP) (0.01 psf) Modified epoxy film adhesive for bonding metallic and composite components

PHEXC437 / 99256

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.