MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay FM® 377U psf 0.055 (269 gsm) Adhesive Film
Categories: Polymer; Adhesive; Film; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: FM® 377 film adhesive is a 350°F (177°C) cure modified epoxy designed for continuous services at 350°F (177°C). FM 377 film adhesive provides outstanding durability in bonding metallic and non-metallic substrates, and in the co-cure or secondary bonding of composites structures. FM 377 adhesive exhibits excellent structural performance from -67°F to 350°F (-55°C to 177°C). FM 377 adhesive is manufactured as a supported film with a knit carrier or as an unsupported film. The unsupported version can be easily reticulated on honeycomb core or perforated metal.

Features & Benefits:

  • Designed for bonding metallic, non-metallic and sandwich structures
  • Excellent combination of high peel strength and high 350°F (177°C) shear strength
  • Designed for continuous service at 350°F (177°C)
  • Superior performance in co-cure or secondary bonding of composite structures
  • Easily reticulated on core or perforated metal for nacelle bonding applications
  • 30 days shop life at 75°F (24°C)
Applications:
  • Bonding metallic, non-metallic and sandwich structures
  • Co-cure and secondary bonding of composite structures

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.0 %<= 1.0 %
Storage Temperature -18.0 °C-0.400 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  2.83 MPa
@Temperature 177 °C
410 psi
@Temperature 351 °F
Flatwise, Honeycomb Specimens
 3.17 MPa
@Temperature 177 °C
460 psi
@Temperature 351 °F
Flatwise, After 1000 hr aging at 350°F (177°C), Honeycomb Specimens
 8.62 MPa
@Temperature 24.0 °C
1250 psi
@Temperature 75.2 °F
Flatwise, Honeycomb Specimens
Shear Strength 5.76 MPa835 psiBeam, Honeycomb Specimens
 13.1 MPa
@Temperature 177 °C
1900 psi
@Temperature 351 °F
Wide Area Lap, Prebond Film Exposure at 24°C, for 63 days
 13.4 MPa
@Temperature 177 °C
1950 psi
@Temperature 351 °F
Wide Area Lap, Prebond Film Exposure at 24°C
 13.96 MPa
@Temperature 177 °C
2025 psi
@Temperature 351 °F
Blister, Metal-to-Metal
 14.10 MPa
@Temperature 177 °C
2045 psi
@Temperature 351 °F
Wide Area Lap, Prebond Film Exposure at 24°C, for 28 days
 14.38 MPa
@Temperature 177 °C
2085 psi
@Temperature 351 °F
Blister, after 1000 hrs at 350°F, Metal-to-Metal
 14.44 MPa
@Temperature 177 °C
2095 psi
@Temperature 351 °F
Wide Area Lap, Prebond Film Exposure at 24°C, for 14 days
 24.9 MPa
@Temperature 24.0 °C
3610 psi
@Temperature 75.2 °F
Wide Area Lap, Prebond Film Exposure at 24°C, for 63 days
 25.06 MPa
@Temperature -55.0 °C
3635 psi
@Temperature -67.0 °F
Wide Area Lap, Prebond Film Exposure at 24°C, for 63 days
 25.5 MPa
@Temperature -55.0 °C
3700 psi
@Temperature -67.0 °F
Blister, Metal-to-Metal
 25.68 MPa
@Temperature -55.0 °C
3725 psi
@Temperature -67.0 °F
Wide Area Lap, Prebond Film Exposure at 24°C, for 28 days
 25.7 MPa
@Temperature -55.0 °C
3730 psi
@Temperature -67.0 °F
Wide Area Lap, Prebond Film Exposure at 24°C, for 14 days
 26.2 MPa
@Temperature -55.0 °C
3800 psi
@Temperature -67.0 °F
Wide Area Lap, Prebond Film Exposure at 24°C
 26.86 MPa
@Temperature 24.0 °C
3895 psi
@Temperature 75.2 °F
Wide Area Lap, Prebond Film Exposure at 24°C, for 28 days
 27.2 MPa
@Temperature 24.0 °C
3940 psi
@Temperature 75.2 °F
Wide Area Lap, Prebond Film Exposure at 24°C, for 14 days
 27.2 MPa
@Temperature 24.0 °C
3950 psi
@Temperature 75.2 °F
Blister, Metal-to-Metal
 27.75 MPa
@Temperature 24.0 °C
4025 psi
@Temperature 75.2 °F
Wide Area Lap, Prebond Film Exposure at 24°C
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C351 °Fcontinuous
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorGrey
Honeycomb Sandwich Peel45 Nm/mPrebond Film Exposure at 24°C, for 28 days
 50 Nm/mPrebond Film Exposure at 24°C
 52 Nm/mHoneycomb Specimens
 53 Nm/mPrebond Film Exposure at 24°C, for 14 days
 54 Nm/mPrebond Film Exposure at 24°C, for 63 days
Metal-to-Metal Climbing Drum Peel124 Nm/mPrebond Film Exposure at 24°C, for 28 days
 129 Nm/mPrebond Film Exposure at 24°C, for 63 days
 129 Nm/mPrebond Film Exposure at 24°C, for 14 days
 133 Nm/mMetal-to-Metal
 142 Nm/mPrebond Film Exposure at 24°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay FM® 377S Adhesive Film, psf 0.08 (391 gsm)
Solvay HTA® 240 Adhesive Film
Solvay FM® 94K Adhesive Film
Phosphorus (V) Sulfide Trifluoride, PSF3
Hexcel® Redux® 340U(SP) (0.01 psf) Modified epoxy film adhesive for bonding metallic and composite components

PCYTED118 / 180420

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.