MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Atom Adhesives AA-BOND FDA15 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-BOND FDA15 is a low viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Administration Chapter 1, Sub Part B, Sections 175.105 and 175.300. AA-BOND FDA15 is two-part adhesive is used for bonding, laminating and repair applications by manufacturers of food preparation, processing and packaging equipment, and by manufacturers of catheters, hearing aids, dental products and other biomedical instruments and devices. AA-BOND FDA15 is an effective electrical insulator, and it provides low permeability to gases and vapors and good resistance to water, weather, galvanic action, to petroleum solvents, lubricants and fuels, to mild acids and alkalis, and to many other organic and inorganic compounds.

Appearance: Clear

Cure Type: Heat cure or Room Temperature

Benefits:

  • Low viscosity
  • Effective electrical insulator
  • Low permeability
  • Good resistance
Mix Ratio by weight: 100:20/Resin:Hardener

Substrates: Most metals, ceramic, glass and plastics

Typical Application: Developed for bonding and coating applications.

Information provided by Atom Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccuncured
Solids Content 100 %100 %reactive, uncured
Volatile Organic Compounds (VOC) Content 3.0 g/l3.0 g/luncured
Viscosity 4500 cP4500 cPuncured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888
Elongation at Yield 4.0 %4.0 %
Shear Strength 13.8 MPa2000 psiLap, Alum to Alum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cm
Dielectric Constant 4.3
@Frequency 1000 Hz
4.3
@Frequency 1000 Hz
Dielectric Strength 16.5 kV/mm420 kV/in
Dissipation Factor 0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.1 µm/m-°C30.6 µin/in-°F
Maximum Service Temperature, Air 140 °C284 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
Glass Transition Temp, Tg 100 °C212 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 240 min
@Temperature 65.0 °C
1.00 - 4.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 25.0 min25.0 minuncured
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Thixotropic Index1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Atom Adhesives AA-BOND F253 Epoxy Adhesive
Atom Adhesives AA-BOND F112 Epoxy Adhesive
Resin Technology Group EN 239-2 Cationic UV Cure Epoxy Adhesive
Master Bond EP17HT-3 One component, snap-curing epoxy system
3M Scotch-Weld™ DP100 FR Epoxy Adhesive

PATOM025 / 172340

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.