MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond EP17HT-3 One component, snap-curing epoxy system
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Product Description: Master Bond Polymer System EP17HT-3 is a one part epoxy that fully cures in 2-3 minutes at 250-300°F. It is capable of service up to +400°F with excellent strength retention properties. Also, unlike many other one part epoxies, EP17HT-3 can be cured in sections up to ¼ inch thick. EP17HT-3 is 100% reactive and contains no solvents or diluents. As a one part system, it not only requires no mixing, but the working life is “indefinite”. It will not gel until heated above 200°F. EP17HT-3 has excellent electrical insulation characteristics, superior chemical resistance and outstanding physical properties. It is yellow to brown in color. There is a paste version called EP17HT-3ND2 as well as a slightly toughened formulation called Supreme 17HT-3 which offers enhanced resistance to thermal cycling and thermal and mechanical shock.

Product Advantages:

  • One part system; no mixing required; contains no solvents or diluents
  • Snap cure: Sets up in 20-30 seconds and fully cures in 2-3 minutes at 250-300°F
  • Superior temperature resistance; serviceable up to +400°F
  • Outstanding electrical insulation properties and chemical resistance
  • Can cure in sections up to ¼ inch thick
  • Easy application: Unlimited working life—will not set up at room temperature

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Viscosity 80000 - 130000 cP80000 - 130000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 85>= 85
Tensile Strength at Break >= 55.2 MPa>= 8000 psi
Shear Strength >= 14.5 MPa>= 2100 psitensile lap, aluminum to aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 4.8
@Frequency 60 Hz,
Temperature 25.0 °C
4.8
@Frequency 60 Hz,
Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.00 - 5.00 µm/m-°C2.22 - 2.78 µin/in-°F
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Glass Transition Temp, Tg 110 - 120 °C230 - 248 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  1.80 - 3.00 min
@Temperature 149 °C
0.0300 - 0.0500 hour
@Temperature 300 °F
 3.00 - 4.02 min
@Temperature 121 °C
0.0500 - 0.0670 hour
@Temperature 250 °F
Shelf Life 6.00 Month6.00 Monthin original, unopened containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting
Master Bond Supreme 42HT-2 Toughened Epoxy Resists Thermal Cycling
Solvay MTM® 23 Vinyl Hybrid Prepreg
Cookson Group Plaskon® SMT-B-1RC Molding Compound for PBGAs
Solvay XMTR50 (EF7313) Epoxy Resin System

PMASTB303 / 149550

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.