MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Total 3802 YCF MDPE pipe grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process.

FINATHENE® 3802 Y CF is a yellow cadmium free polyethylene specially developed for the manufacture of pressure pipes and fittings and accessories for gas distribution networks.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D 792
Viscosity 1.30e+6 cP
@Shear Rate 100 1/s,
Temperature 190 °C
1.30e+6 cP
@Shear Rate 100 1/s,
Temperature 374 °F
ATOFINA research test
Environmental Stress Crack Resistance >= 700 hour>= 700 hourASTM D1693
Oxidative Induction Time (OIT) >= 20 min>= 20 min210°C; EN 728
 >= 30 min>= 30 min200°C; EN 728
Melt Flow  0.20 g/10 min
@Load 2.16 kg
0.20 g/10 min
@Load 4.76 lb
ASTM D 1238
 0.92 g/10 min
@Load 5.00 kg
0.92 g/10 min
@Load 11.0 lb
ASTM D 1238
High Load Melt Index 18 g/10 min
@Load 21.6 kg
18 g/10 min
@Load 47.6 lb
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060DIN 53505
Tensile Strength at Break 32.0 MPa4640 psiISO 527
Tensile Strength, Yield 18.0 MPa2610 psiISO 527
Elongation at Break >= 700 %>= 700 %ISO R527
Elongation at Yield 9.0 %9.0 %ISO 527
Modulus of Elasticity 0.700 GPa102 ksiISO 178
Flexural Modulus 0.700 GPa102 ksiASTM D 790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmIEC 93
Surface Resistance >= 1.00e+16 ohm>= 1.00e+16 ohmIEC 93
Dielectric Constant 2.35
@Frequency 1000 Hz
2.35
@Frequency 1000 Hz
IEC 250
Dielectric Strength 16.0 kV/mm406 kV/inIEC 243
Dissipation Factor 0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
IEC 250
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 160 J/g68.8 BTU/lbDSC
Specific Heat Capacity 2.00 J/g-°C0.478 BTU/lb-°FDSC
 2.60 J/g-°C
@Temperature 150 °C
0.621 BTU/lb-°F
@Temperature 302 °F
DSC
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°FDIN 52612
 0.200 W/m-K
@Temperature 150 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 302 °F
DIN 52612
Melting Point 125 - 129 °C257 - 264 °Fcrystalline; DSC
Vicat Softening Point 125 °C257 °FISO 306
Brittleness Temperature -100 °C-148 °FASTM D 746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos K38-20-188 HDPE
Ineos K38-20-160 Polyethylene Copolymer
LyondellBasell Alathon® L5005V High Density Polyethylene, HMW Film Grade
NOVA Chemicals Novapol® HD-2100-U MDPE Extrusion Resin
Total HP 401N Natural HDPE, pipe

PFINAP113 / 38696

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.