MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kohesi Bond KB 1048 FLAO Two component, flexible, room temperature curing, thermally conductivity epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Product Highlights:
  • Superior thermal conductivity
  • Excellent flow properties
  • First-rate flexibility
  • Very low exotherm, ideal for casting
  • Exceptional electrical insulation properties
  • Resists mechanical and thermal shocks
Kohesi Bond KB 1048 FLAO is a two component, room temperature curing epoxy system suitable for bonding, sealing, potting and encapsulation. It has a convenient 1:1 (Part A: Part B) mix ratio by weight or volume. This epoxy system offers excellent flexibility and peel strength. It readily cures at room temperature and can achieve faster cures at elevated temperatures. The optimal cure schedule is an overnight room temperature set-up followed by a heat cure at 70°C - 90°C for 3 - 5 hours. KB 1048 FLAO is thermally conductive and offers top notch heat transfer properties. It offers an extensive service temperature range of -73°C to +120°C. This adhesive fosters outstanding resistance to mechanical and thermal shocks. It is a 100% solids system, offering minimal shrinkage upon cure. KB 1048 FLAO adheres well to a wide variety of substrates including metals, ceramics, most plastics and glass. In addition to superior electrical insulation, it also offers lower exotherm, making it ideal for stress free bonding. Part A and Part B are light gray in color. KB 1048 FLAO is widely used in optoelectronic, electronics, automotive, space and related industries especially where thermal conductivity and high flexibility are desired.

Typical Applications:

  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors: Kohesi Bond is a pioneer in manufacturing over 300 grades of custom engineered adhesives, sealants, coatings, potting and encapsulation compounds. Our first-rate adhesives are tailor-fitted to meet your exact specifications and offer superior strength and performance in your application. Learn more about Kohesi Bond’s industry-ready products at kohesibond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 6000 - 20000 cP6000 - 20000 cPPart B
 20000 - 80000 cP20000 - 80000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 30 - 5030 - 50
Tensile Strength >= 28.3 MPa>= 4100 psi
Tensile Modulus 0.379 - 0.758 GPa55.0 - 110 ksi
Adhesive Bond Strength >= 6.21 MPa>= 900 psiTensile Lap Shear, Al/Al
Peel Strength >= 1.75 kN/m>= 10.0 pliT-peel Strength, Al/Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Dielectric Constant 4.81
@Frequency 60 Hz
4.81
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 - 65.0 µm/m-°C33.3 - 36.1 µin/in-°F
Thermal Conductivity 1.30 - 1.40 W/m-K9.02 - 9.72 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 120 °C248 °F
Minimum Service Temperature, Air -73.0 °C-99.4 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  150 - 210 min
@Temperature 90.0 °C
2.50 - 3.50 hour
@Temperature 194 °F
Option 2
 180 - 300 min
@Temperature 70.0 - 90.0 °C
3.00 - 5.00 hour
@Temperature 158 - 194 °F
Optimum Cure: overnight at 23°C plus 3 - 5 hours at 70°C - 90°C
 2880 - 4320 min
@Temperature 23.0 °C
48.0 - 72.0 hour
@Temperature 73.4 °F
Option 1
Working Life 50.0 - 150 min50.0 - 150 min100 g of mixed epoxy
Shelf Life 12.0 Month12.0 Monthin original unopened containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKOHESI926 / 249105

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.