MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Adaptive3D Elastic ToughRubber™ 90 (ETR 90) Elastomer for DLP
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Adaptive3D Elastic ToughRubber™ 90 (ETR 90) is an elastomeric material with a tough, rubber-like performance, allowing for the 3D printing of parts previously made from technical foams, rubbers, or polyurethanes. E-RE90 is one of the toughest elastomers on the market with high performance that is ideal for a multitude of end parts, products, and functional prototypes such as midsoles, heel cups, seals, and door boots, foam-like lattice structuring, or tough enclosures. It is also recommended for vibration isolation parts due to its extraordinary damping properties.

Applications: manufacturing, consumer goods, automotive, aerospace, foam replacement, seals and gaskets.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.038 g/cc0.03750 lb/in³Liquid
Viscosity 7900 cP7900 cPLiquid as Supplied
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9292ASTM D2240
Tensile Strength, Ultimate 14.0 MPa2030 psi
Elongation at Break 190 %190 %ASTM D638 Type V
Tensile Modulus 0.0590 GPa8.56 ksiStorage; ASTM D4065
Resilience 4949% Bayshore
 49.049.0[%], Bayshore; ASTM D2632
Tear Strength 38.0 kN/m217 pli
Compression Set  25.0 %
@Treatment Temp. 25.0 °C,
Time 79200 sec
25.0 %
@Treatment Temp. 77.0 °F,
Time 22.0 hour
ASTM D395 Method B Type 1
 53.0 %
@Treatment Temp. 70.0 °C,
Time 79200 sec
53.0 %
@Treatment Temp. 158 °F,
Time 22.0 hour
ASTM D395 Method B Type 1
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -62.0 °C-79.6 °FDMA. Low
 86.0 °C187 °FDMA. High
 
Descriptive Properties
Bio-Compatibility TestingPassedCyotoxicity (ISO 10993-5)
 PassedIrritation (ISO 10993-10)
 PassedSensitization (ISO 10993-5)
ColorBlack
Fracture Toughness17.9 MJ/m^3ASTM D638 Type V
Fracture Toughness (MJ/m3)17.9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PADAPT92 / 305369

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.