Features: Outstanding resiliency, fuel resistance and low temperature flexibility. Uses: Hose and Tube, Injection Molding, Fabric Coating and Wire/Cable Available in Americas, Europe, Middle East, Africa, India and Asia Information Provided by The Lubrizol Corporation |