MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol LifeSciences Carbothane® AC-4095A TPU – Clear Aromatic
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Medical Grade Aromatic Polycarbonate-based Thermoplastic Polyurethane (TPU)

Features: good mechanical properties, good chemical resistance, excellent oxidative stability and biocompatibility properties and can be color-matched

Process: Extrusion and Injection Molding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/in1”x.25”x6” bar; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595ASTM D785
Tensile Strength, Ultimate 68.9 MPa10000 psiASTM D412
Elongation at Break 370 %370 %ASTM D412
100% Modulus 14.65 MPa
@Strain 100 %
2125 psi
@Strain 100 %
ASTM D412
200% Modulus 32.8 MPa
@Strain 200 %
4750 psi
@Strain 200 %
ASTM D412
300% Modulus 53.1 MPa
@Strain 300 %
7700 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.0745 GPa10.8 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 124 °C255 °FASTM D1525
Glass Transition Temp, Tg -10.0 °C14.0 °F
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 205 °C401 °FInjection
Front Barrel Temperature 210 °C410 °FInjection
Nozzle Temperature 215 °C419 °FInjection
Zone 1 210 °C410 °FExtrusion
Zone 2 215 °C419 °FExtrusion
Zone 3 221 °C430 °FExtrusion
Zone 4 221 °C430 °FExtrusion
Adapter Temperature 215 °C419 °FExtrusion
Die Temperature 215 °C419 °FExtrusion
Melt Temperature 210 °C410 °FInjection
Mold Temperature 10.0 - 27.0 °C50.0 - 80.6 °FInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Carbothane® PC-3595A TPU – Clear Aliphatic
Covestro Desmopan® DP 8410 Polyurethane
Lubrizol Advanced Materials PEARLTHANE® 11T93 Thermoplastic Polyurethane Elastomer
Lubrizol Estane® 58070 Thermoplastic Polyurethane
Lubrizol LifeSciences Carbothane® AC-4085A TPU – Clear Aromatic

PLUBR9013 / 203580

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.