MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Borealis Borseal™ TD218BF Terpolymer for BOPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP)

Material Notes: Borseal TD218BF is a C2/C4 terapolymer film resin.

Borseal TD218BF is especially developed for use as sealing layers in coextruded BOPP film (manufactured on Stenter frame and double bubble film processes).

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus 0.700 GPa102 ksiISO 178
Heat Seal Strength Initiation Temperature 103 °C217 °F3 N; Borealis Test
 
Thermal PropertiesMetricEnglishComments
Melting Point 128 - 132 °C262 - 270 °FISO 3146
Vicat Softening Point 114 °C237 °F10 N; ISO 306A
 
Optical PropertiesMetricEnglishComments
Haze 1.0 %1.0 %Borealis Test

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 COPYLENE® CH020-01 Polypropylene, Homopolymer, BOPP
Overview of materials for Polypropylene, Molded
Overview of materials for Polypropylene, Blow Molding Grade
Formosa Plastics Formolene® 1102K Cast and BOPP Film Polypropylene
DuPont Teijin Films Mylar® RL31 Polyester Film, 50 Gauge

PBOREA099 / 27406

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.