MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polypropylene, Blow Molding Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.886 - 2.00 g/cc0.0320 - 0.0723 lb/in³Average value: 0.915 g/cc Grade Count:112
Oxygen Transmission 95.0 cc-mm/m²-24hr-atm241 cc-mil/100 in²-24hr-atmAverage value: 95.0 cc-mm/m²-24hr-atm Grade Count:10
Linear Mold Shrinkage 0.0100 - 0.0250 cm/cm0.0100 - 0.0250 in/inAverage value: 0.0174 cm/cm Grade Count:7
Melt Flow 0.250 - 1900 g/10 min0.250 - 1900 g/10 minAverage value: 83.3 g/10 min Grade Count:135
Ash 0.0200 - 0.120 %0.0200 - 0.120 %Average value: 0.0583 % Grade Count:6
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 61.0 - 11261.0 - 112Average value: 87.7 Grade Count:87
Hardness, Shore D 61.0 - 73.061.0 - 73.0Average value: 68.7 Grade Count:6
Tensile Strength, Ultimate 17.9 - 35.0 MPa2600 - 5080 psiAverage value: 26.7 MPa Grade Count:18
Film Tensile Strength at Yield, MD 27.0 - 47.0 MPa3920 - 6820 psiAverage value: 35.0 MPa Grade Count:3
Film Tensile Strength at Yield, TD 23.0 - 32.0 MPa3340 - 4640 psiAverage value: 27.5 MPa Grade Count:3
Tensile Strength, Yield 17.0 - 42.3 MPa2470 - 6140 psiAverage value: 30.2 MPa Grade Count:111
Film Elongation at Break, MD 580 - 700 %580 - 700 %Average value: 630 % Grade Count:3
Film Elongation at Break, TD 280 - 850 %280 - 850 %Average value: 593 % Grade Count:3
Elongation at Break 3.00 - 700 %3.00 - 700 %Average value: 225 % Grade Count:57
Elongation at Yield 2.50 - 20.0 %2.50 - 20.0 %Average value: 10.8 % Grade Count:88
Modulus of Elasticity 0.750 - 1.80 GPa109 - 261 ksiAverage value: 1.20 GPa Grade Count:29
Flexural Yield Strength 25.0 - 49.0 MPa3630 - 7110 psiAverage value: 36.6 MPa Grade Count:12
Flexural Modulus 0.689 - 3.70 GPa99.9 - 537 ksiAverage value: 1.27 GPa Grade Count:113
Secant Modulus, MD 0.680 - 0.896 GPa98.6 - 130 ksiAverage value: 0.795 GPa Grade Count:3
Secant Modulus, TD 0.650 - 0.790 GPa94.3 - 115 ksiAverage value: 0.737 GPa Grade Count:3
Izod Impact, Notched 0.140 - 5340 J/cm0.262 - 10000 ft-lb/inAverage value: 1.60 J/cm Grade Count:97
 0.170 - 3.98 J/cm
@Temperature -20.0 - 3.89 °C
0.318 - 7.46 ft-lb/in
@Temperature -4.00 - 39.0 °F
Average value: 0.858 J/cm Grade Count:16
Izod Impact, Notched (ISO) 2.79 - 56.0 kJ/m²1.33 - 26.6 ft-lb/in²Average value: 20.7 kJ/m² Grade Count:6
 2.604 - 4.20 kJ/m²
@Temperature -40.0 - 3.89 °C
1.239 - 2.00 ft-lb/in²
@Temperature -40.0 - 39.0 °F
Average value: 3.47 kJ/m² Grade Count:3
Charpy Impact, Notched 0.200 - 55.0 J/cm²0.952 - 262 ft-lb/in²Average value: 5.37 J/cm² Grade Count:18
 0.400 - 12.0 J/cm²
@Temperature -20.0 - 0.000 °C
1.90 - 57.1 ft-lb/in²
@Temperature -4.00 - 32.0 °F
Average value: 3.54 J/cm² Grade Count:6
Gardner Impact 28.0 - 36.6 J20.7 - 27.0 ft-lbAverage value: 34.9 J Grade Count:18
 1.00 - 1.00 J
@Temperature -30.0 - 0.000 °C
0.738 - 0.738 ft-lb
@Temperature -22.0 - 32.0 °F
Average value: 30.2 J Grade Count:5
Tangent Modulus 869 - 1300 MPa126000 - 189000 psiAverage value: 1020 MPa Grade Count:3
 
Thermal PropertiesMetricEnglishComments
Melting Point 132 - 165 °C270 - 329 °FAverage value: 151 °C Grade Count:39
Deflection Temperature at 0.46 MPa (66 psi) 71.0 - 133 °C160 - 271 °FAverage value: 91.3 °C Grade Count:119
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 60.0 °C113 - 140 °FAverage value: 54.1 °C Grade Count:7
Vicat Softening Point 67.0 - 160 °C153 - 320 °FAverage value: 140 °C Grade Count:19
 
Optical PropertiesMetricEnglishComments
Haze 0.600 - 71.0 %0.600 - 71.0 %Average value: 17.1 % Grade Count:23
Gloss 80.0 - 110 %80.0 - 110 %Average value: 95.8 % Grade Count:5
Transmission, Visible 18.5 - 90.0 %18.5 - 90.0 %Average value: 44.8 % Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 230 °C356 - 446 °FAverage value: 203 °C Grade Count:6
Melt Temperature 177 - 250 °C351 - 482 °FAverage value: 215 °C Grade Count:21
Head Temperature 210 °C410 °FAverage value: 210 °C Grade Count:5
Mold Temperature 16.0 °C60.8 °FAverage value: 16.0 °C Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Molded
Overview of materials for Polypropylene, Extrusion Grade
Overview of materials for Polypropylene, Film Grade
Overview of materials for Polypropylene with 10% Glass Fiber Filler
Overview of materials for Polypropylene with 20% Glass Fiber Filler

O4706 / 78373

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.