Pump Oil is a highly refined paraffinic mineral oil developed for drip-feed lubrication of deep-well turbine water pumps. Pump Oil is a highly refined, non-compounded paraffinic mineral oil. It contains no hazardous additives that can affect water quality, and has negligible odor. Applications: - Deep-well water pumps for domestic and agricultural use
- Vacuum pumps
- Industrial applications that require a non-compounded, ISO VG 46 mineral oil
Features/Benefits:- Contains no hazardous additives
- Low odor
- Good low-temperature properties
Information provided by Phillips 66 Lubricants. |