MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dow 702 DIFFUSION PUMP FLUID
Categories: Fluid; Polymer; Thermoplastic; Siloxane

Material Notes: Former Dow Corning product.

Information provided by Dow Corning

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc
@Temperature 25.0 °C
1.07 g/cc
@Temperature 77.0 °F
Viscosity Measure 45 cSt45 cStkinetic/kinematic
Surface Tension 30 dynes/cm30 dynes/cm
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 90800 J/g
@Temperature 190 °C
39100 BTU/lb
@Temperature 374 °F
Boiling Point 180 °C356 °F
Flash Point 193 °C379 °Fopen cup
 
Processing PropertiesMetricEnglishComments
Shelf Life 60.0 Month60.0 Month
 
Descriptive Properties
Ultimate Vacuum (Torr)1E-06untrapped

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow 520 DILUTABLE WATER REPELLENT
Dow Z-6689 WATER REPELLENT
Elmet-Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy
Overview of materials for Silicone Rubber
CHT Group QSil 1000 43 Shore A, Addition Cure, Self-Bonding, One Part Siloxane Elastomer

PDOWCO627 / 106328

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.