MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Polyram RamSter PF100 PBT, General Purpose
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: General purpose, high viscosity PBT for injection molding applications

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³DIN 53479
Water Absorption 0.60 %0.60 %DIN 53495
Moisture Absorption at Equilibrium 0.25 %0.25 %23° C, 50% RH; DIN 53714
Linear Mold Shrinkage 0.023 cm/cm0.023 in/in
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 57.0 MPa8270 psiASTM-D638
Elongation at Break 30 %30 %ASTM-D638
Flexural Strength 85.0 MPa12300 psiASTM D790
Flexural Modulus 2.20 GPa319 ksiASTM-D790
Izod Impact, Notched 0.400 J/cm
@Temperature 23.0 °C
0.749 ft-lb/in
@Temperature 73.4 °F
ASTM-D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmDIN 53482
Dielectric Constant 3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
VDE 0303/4
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °F
Deflection Temperature at 0.46 MPa (66 psi) 170 °C338 °FDIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FDIN 53461
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Glow Wire Test 750 °C1380 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chem Polymer Durlex 700 PBT, General Purpose
Overview of materials for Polyetheretherketone, Unreinforced
Mitsubishi Chemical Advanced Materials Nylatron™ 101 / Ertalon™ 66 SA PA66 Extruded, Unfilled, Type 66 Natural and Black
LNP STARAMIDE PF-100-10 HS NAT95 Polyamide 6, Glass Fiber Reinforcement
Ensinger Tecapeek® Polyetheretherketone (PEEK)

PPOLYRA135 / 57397

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.