MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestodur® X7065 Low Viscous PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Description: VESTODUR X7065 is a low-viscous, easy flowing thermoplastic polyester resin based on polybutylene terephthalate. The resin is especially suitable for the manufacture of parts according to the melt-blow process which are subjected to high mechanical and thermal load.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccISO 1183
Water Absorption at Saturation 0.50 %ISO 62
Linear Mold Shrinkage 0.015 cm/cm
@Thickness 2.00 mm
sheet with film gate at rim, mold temperature 80°C
Linear Mold Shrinkage, Transverse 0.015 cm/cm
Melt Flow 209.6 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ISO 868
Tensile Strength at Break 55.0 MPaISO 527-1/-2
Elongation at Break 5.0 %ISO 527-1/2
Elongation at Yield 7.0 %Outer fiber strain at maximum stress, 5 mm/min; ISO 178
Tensile Modulus 2.60 GPaISO 527-1/-2
Flexural Strength 70.0 MPaat 3.5% strain, 5 mm/min; ISO 178
 90.0 MPa5 mm/min; ISO 178
Charpy Impact Unnotched 4.00 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
 5.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.250 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 0.300 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.3
@Frequency 100 Hz
IEC 60250
 3.5
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.0020
@Frequency 100 Hz
IEC 60250
 0.023
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 575 V100 drops value; IEC 60112
 600 VTest Solution A CTI; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 µm/m-°C
@Temperature 23.0 - 55.0 °C
Longitudinal; ISO 11359, DIN 53752
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359, DIN 53752
Deflection Temperature at 0.46 MPa (66 psi) 150 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CISO 75-1/-2
Vicat Softening Point 190 °CMethod B, 50 N; ISO 306
 220 °CMethod A, 10 N; ISO 306
Flammability, UL94 HB
@Thickness 0.800 mm
IEC 60695
 HB
@Thickness 1.60 mm
IEC 60695

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical Lupox® TE-5020 High Impact PBT, Thermoplastic Elastomer Alloy, Blow Molding
Lanxess Pocan® B 700 000000 PBT
DuPont Mobility and Materials Crastin® CE2061 BK560 PBT
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded

PHUMA61 / 47575

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.