MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Henkel Loctite® Stycast® ES 0513 Two-Component Epoxy Encapsulant
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Loctite Stycast ES 0513 provides the following product characteristics:

Cure: Heat cure

Application: Potting and Encapsulating

Loctite Stycast ES 0513 is a two-component, filled epoxy system designed for vacuum impregnation applications as well as for general potting and encapsulating.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.74 g/ccPart B
 1.76 g/ccCured
 1.77 g/ccPart A
 1.79 g/ccCured
Solids Content 100 %Part A
 100 %Part B
Filler Content 63 %Part A
 63 %Part B
Brookfield Viscosity 30000 cPPart B; RVF, Spindle 5, speed 4 rpm
 215000 cPPart A; RVF, Spindle 7, speed 10 rpm
Linear Mold Shrinkage 0.0066 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90
Elongation at Break 1.5 %
Tensile Modulus 6550 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.57e+13 ohm-cm
@Temperature 125 °C
 2.50e+16 ohm-cm
@Temperature 23.0 °C
Dielectric Constant 3.8
@Frequency 1000 Hz,
Temperature 23.0 °C
 3.8
@Frequency 10000 Hz,
Temperature 23.0 °C
 4.8
@Frequency 10000 Hz,
Temperature 125 °C
 5.3
@Frequency 1000 Hz,
Temperature 125 °C
Dielectric Strength 1215 V/mil
@Thickness 20.0 mm
Dissipation Factor 0.0043
@Frequency 1000 Hz,
Temperature 23.0 °C
 0.0046
@Frequency 10000 Hz,
Temperature 23.0 °C
 0.0604
@Frequency 10000 Hz,
Temperature 125 °C
 0.0609
@Frequency 1000 Hz,
Temperature 125 °C
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 88.0 °CTMA
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 125 °C
Alternate Cure Schedule, Plus 1 hour @ 150°C
 2.00 hour
@Temperature 93.0 °C
Cure Schedule, Plus 3 hours @ 150°C
Shelf Life 12.0 MonthPart A, From date of manufacture
 12.0 MonthPart B, From date of manufacture
 
Descriptive Properties
AppearanceBlackMixed
 BlackPart B
 GrayPart A
Mix Ratio, by Volume98.4 : 100Part A : Part B
Mix Ratio, by Weight100 : 99.9Component A : Component B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHENK7948 / 255433

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.