MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Henkel Loctite® Stycast® ES 0513 Two-Component Epoxy Encapsulant
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Loctite Stycast ES 0513 provides the following product characteristics:

Cure: Heat cure

Application: Potting and Encapsulating

Loctite Stycast ES 0513 is a two-component, filled epoxy system designed for vacuum impregnation applications as well as for general potting and encapsulating.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.74 g/cc0.0629 lb/in³Part B
 1.76 g/cc0.0636 lb/in³Cured
 1.77 g/cc0.0639 lb/in³Part A
 1.79 g/cc0.0647 lb/in³Cured
Solids Content 100 %100 %Part A
 100 %100 %Part B
Filler Content 63 %63 %Part A
 63 %63 %Part B
Brookfield Viscosity 30000 cP30000 cPPart B; RVF, Spindle 5, speed 4 rpm
 215000 cP215000 cPPart A; RVF, Spindle 7, speed 10 rpm
Linear Mold Shrinkage 0.0066 cm/cm0.0066 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090
Elongation at Break 1.5 %1.5 %
Tensile Modulus 6.55 GPa950 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  5.57e+13 ohm-cm
@Temperature 125 °C
5.57e+13 ohm-cm
@Temperature 257 °F
 2.50e+16 ohm-cm
@Temperature 23.0 °C
2.50e+16 ohm-cm
@Temperature 73.4 °F
Dielectric Constant  3.8
@Frequency 1000 Hz,
Temperature 23.0 °C
3.8
@Frequency 1000 Hz,
Temperature 73.4 °F
 3.8
@Frequency 10000 Hz,
Temperature 23.0 °C
3.8
@Frequency 10000 Hz,
Temperature 73.4 °F
 4.8
@Frequency 10000 Hz,
Temperature 125 °C
4.8
@Frequency 10000 Hz,
Temperature 257 °F
 5.3
@Frequency 1000 Hz,
Temperature 125 °C
5.3
@Frequency 1000 Hz,
Temperature 257 °F
Dielectric Strength 47.83 kV/mm
@Thickness 20.0 mm
1215 kV/in
@Thickness 0.787 in
Dissipation Factor  0.0043
@Frequency 1000 Hz,
Temperature 23.0 °C
0.0043
@Frequency 1000 Hz,
Temperature 73.4 °F
 0.0046
@Frequency 10000 Hz,
Temperature 23.0 °C
0.0046
@Frequency 10000 Hz,
Temperature 73.4 °F
 0.0604
@Frequency 10000 Hz,
Temperature 125 °C
0.0604
@Frequency 10000 Hz,
Temperature 257 °F
 0.0609
@Frequency 1000 Hz,
Temperature 125 °C
0.0609
@Frequency 1000 Hz,
Temperature 257 °F
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 88.0 °C190 °FTMA
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 125 °C
2.00 hour
@Temperature 257 °F
Alternate Cure Schedule, Plus 1 hour @ 150°C
 120 min
@Temperature 93.0 °C
2.00 hour
@Temperature 199 °F
Cure Schedule, Plus 3 hours @ 150°C
Shelf Life 12.0 Month12.0 MonthPart A, From date of manufacture
 12.0 Month12.0 MonthPart B, From date of manufacture
 
Descriptive Properties
AppearanceBlackMixed
 BlackPart B
 GrayPart A
Mix Ratio, by Volume98.4 : 100Part A : Part B
Mix Ratio, by Weight100 : 99.9Component A : Component B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHENK7948 / 255433

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.