MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Blue River Coatings Acrylic 4000 Topcoat
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a hard, flexible, economical coating designed for multiple substrates. BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT offers good application properties, low foam, good adhesion, and high gloss potential. ACRYLIC 4000 TOPCOAT dries quickly (eliminating excessive grain raise on wood) and provides good sealing to help repel water. The product is designed to work in conjunction with Blue River Coatings Wood Stains and Primers.

Enviromental Advantages:BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a low VOC (Volatile Organic Compound), performance production coating. It is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with your local and state regulations for proper handling.

Characteristics:

  • Low cost coating
  • Good hardness/impact resistance
  • Good Solvent resistance-20 double rub MEK with little to no effect
  • Excellent water resistance – 1 hour covered water spot test: No spotting or discoloration
  • Good alcohol resistance –1 hour covered alcohol spot test: 50% isopropyl – slight whitening, 70% isopropyl – slight whitening
  • High solids
  • Available in satin to gloss finish
  • Can be applied in a wide variety of temperature and humidity conditions
  • Air drying or force curing preferred
  • Water is used for clean-up
  • Non-Hazardous
  • Non-Flammable
  • Shelf life of 1 year
  • Uses

  • Wood
  • Steel
  • Aluminum
  • Some Plastics
  • Information provided by Blue River Coatings

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity >= 1.00 g/cc
    Density 8.60 lb/gal
    Solids Content 39.8 %by volume
     45 %by weight
    Volatile Organic Compounds (VOC) Content 228 g/l
     
    Thermal PropertiesOriginal ValueComments
    Boiling Point 93.0 °C
    Flash Point 150 °F
     
    Processing PropertiesOriginal ValueComments
    Cure Time 0.0500 - 0.0830 hour
    @Temperature 75.0 °C
    Recoat, at 50% humidity
     0.0830 hour
    @Temperature 75.0 °C
    Dust Free, at 50% humidity
     0.133 - 0.167 hour
    @Temperature 75.0 °C
    Dry to handle, at 50% humidity and 75°C
    Shelf Life 12.0 Month
     
    Descriptive Properties
    FlexibilityGood
    Pencil HardnessHB
    Salt SprayGood
    Solvent ResistanceGood
    Theoretical Coverage638 ft2 at 1 mil

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    BYK Optiflo® T1000 (Formerly RXL-7301) Polymer
    Bostik Tube & Tile Caulk Siliconized-Acrylic Caulk
    Saint-Gobain Normount® V2800 Energy-Dissipating High-Performance Polyurethane Foam with Acrylic Adhesive
    Mallard Creek Polymers Rovene® 6087 Styrene-Acrylic Emulsion
    Lucite International Series 500 Liquid Acrylic Resin

    WBLUER05 / 74604

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.