MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mallard Creek Polymers Rovene® 6087 Styrene-Acrylic Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: ROVENE® 6087 is a high solids, low VOC styrene-acrylic copolymer emulsion that provides outstanding wet strength and moisture barrier properties.
APPLICATIONS: ROVENE® 6087 typical applications are for use in coatings where moisture barrier properties are important.

Information provided by Mallard Creek Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 56 - 58 %56 - 58 %
Particle Size 0.20 µm0.20 µm
pH 7.0 - 8.07.0 - 8.0
Brookfield Viscosity 400 - 1000 cP400 - 1000 cP#2/20 rpm
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 7.00 °C44.6 °F
 
Descriptive Properties
EmulsifiersAnionic
Residual Monomer0.02% Max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Optiflo® T1000 (Formerly RXL-7301) Polymer
Bostik Tube & Tile Caulk Siliconized-Acrylic Caulk
Blue River Coatings Acrylic 4000 Topcoat
Saint-Gobain Normount® V2800 Energy-Dissipating High-Performance Polyurethane Foam with Acrylic Adhesive
Lucite International Series 500 Liquid Acrylic Resin

PMCP010 / 104667

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.