MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ineos ABS Lustran® LK197 ABS, Extrusion Grade  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as excellent melt strength for good thermoformability. It is easy to color with ABS color concentrates. Lustran® ABS LK197 resin is used for applications that require high gloss and higher rigidity, such as bathtubs, sinks, and shower surrounds for recreational vehicles, and interior liners for ice chests and picnic coolers.

Lustran® is now a product of INEOS Styrolution. Information provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccASTM-D792
Water Absorption 0.40 %
@Time 86400 sec
ASTM-D570
Melt Flow 9.2 g/10 min
@Load 10.0 kg,
Temperature 230 °C
ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 113ASTM-D785
Tensile Strength, Yield 22.1 MPa
@Temperature 71.0 °C
ASTM-D638
 40.0 MPa
@Temperature 23.0 °C
ASTM-D638
 59.3 MPa
@Temperature -18.0 °C
ASTM-D638
Tensile Modulus 1.50 GPa
@Temperature 71.0 °C
ASTM-D638
 2.30 GPa
@Temperature 23.0 °C
ASTM-D638
 2.60 GPa
@Temperature -18.0 °C
ASTM-D638
Flexural Yield Strength 49.6 MPa
@Temperature 71.0 °C
ASTM-D790
 63.4 MPa
@Temperature 23.0 °C
ASTM-D790
 113.8 MPa
@Temperature -40.0 °C
ASTM-D790
Flexural Modulus 1900 MPa
@Temperature 71.0 °C
ASTM-D790
 2500 MPa
@Temperature 23.0 °C
ASTM-D790
 2800 MPa
@Temperature -40.0 °C
ASTM-D790
Izod Impact, Notched 91.0 J/m
@Thickness 3.20 mm,
Temperature -40.0 °C
ASTM-D256
 133 J/m
@Thickness 3.20 mm,
Temperature -18.0 °C
ASTM-D256
 240 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM-D256
Instrumented Impact Total Energy 14.0 J
@Temperature -40.0 °C
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); ASTM-D3763
 24.0 J
@Temperature -18.0 °C
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); ASTM-D3763
 30.0 J
@Temperature 23.0 °C
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); ASTM-D3763
Instrumented Impact Energy at Peak 11.0 J
@Temperature -40.0 °C
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); ASTM-D3763
 19.0 J
@Temperature -18.0 °C
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); ASTM-D3763
 22.0 J
@Temperature 23.0 °C
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); ASTM-D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°CASTM-D696
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °CUnannealed; ASTM-D648
 101 °CAnnealed; ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °CUnannealed; ASTM-D648
 94.0 °CAnnealed; ASTM-D648
UL RTI, Electrical 60.0 °C
@Thickness 1.50 mm
UL746B
UL RTI, Mechanical with Impact 60.0 °C
@Thickness 1.50 mm
UL746B
UL RTI, Mechanical without Impact 60.0 °C
@Thickness 1.50 mm
UL746B
Flammability, UL94 HB
@Thickness 1.47 mm
Flame Spread 35.6 mm/min
@Thickness 3.20 mm
ASTM-D635
 
Optical PropertiesOriginal ValueComments
Gloss 90 %Angle 60°, Sheet; ASTM-D523
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 215 - 240 °CExtrusion
Middle Barrel Temperature 215 - 240 °CExtrusion
Front Barrel Temperature 215 - 240 °CExtrusion
Die Temperature 210 - 240 °C
Melt Temperature 215 - 249 °CExtrusion
Roll Temperature 63.0 - 85.0 °CDown Stack, Middle
 71.0 - 93.0 °CUp Stack, Bottom
 77.0 - 99.0 °CUp Stack, Middle
 82.0 - 105 °CDown Stack, Bottom
 82.0 - 105 °CUp Stack, Top
 82.0 - 105 °CDown Stack, Top
Drying Temperature 82.0 - 93.0 °C
@Time 10800 - 14400 sec
Moisture Content <= 0.030 %
Dew Point <= -29.0 °Cinlet air
 
Descriptive Properties
Pump Ratio1.5-2.0Extrusion
Screw Compression Ratio2.5-2.7Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asahi Kasei Stylac™ A4130 ABS Polymer, Extrusion
Asahi Kasei Stylac™ AE490 ABS Polymer, Extrusion, High Molding
Asahi Kasei Stylac™ AE510 ABS Polymer, Extrusion, High Molding
Asahi Kasei Stylac™ AE850 ABS Polymer, Extrusion, High Molding
Elix Polymers ELIX ABS E211 LNS013 Acrylonitrile Butadiene Styrene (ABS), Extrusion, Impact Grade

PINEA929 / 107200

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.