Physical Properties | Metric | English | Comments |
---|
Density | 1.06 g/cc | 0.0383 lb/in³ |
Water Absorption | 0.40 % @Time 86400 sec | 0.40 % @Time 24.0 hour |
Melt Flow | 9.2 g/10 min @Load 10.0 kg, Temperature 230 °C | 9.2 g/10 min @Load 22.0 lb, Temperature 446 °F |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Rockwell R | 113 | 113 |
Tensile Strength, Yield | 22.1 MPa @Temperature 71.0 °C | 3210 psi @Temperature 160 °F |
| 40.0 MPa @Temperature 23.0 °C | 5800 psi @Temperature 73.4 °F |
| 59.3 MPa @Temperature -18.0 °C | 8600 psi @Temperature -0.400 °F |
Tensile Modulus | 1.50 GPa @Temperature 71.0 °C | 218 ksi @Temperature 160 °F |
| 2.30 GPa @Temperature 23.0 °C | 334 ksi @Temperature 73.4 °F |
| 2.60 GPa @Temperature -18.0 °C | 377 ksi @Temperature -0.400 °F |
Flexural Yield Strength | 49.6 MPa @Temperature 71.0 °C | 7190 psi @Temperature 160 °F |
| 63.4 MPa @Temperature 23.0 °C | 9200 psi @Temperature 73.4 °F |
| 113.8 MPa @Temperature -40.0 °C | 16510 psi @Temperature -40.0 °F |
Flexural Modulus | 1.90 GPa @Temperature 71.0 °C | 276 ksi @Temperature 160 °F |
| 2.50 GPa @Temperature 23.0 °C | 363 ksi @Temperature 73.4 °F |
| 2.80 GPa @Temperature -40.0 °C | 406 ksi @Temperature -40.0 °F |
Izod Impact, Notched | 0.910 J/cm @Thickness 3.20 mm, Temperature -40.0 °C | 1.70 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
| 1.33 J/cm @Thickness 3.20 mm, Temperature -18.0 °C | 2.49 ft-lb/in @Thickness 0.126 in, Temperature -0.400 °F |
| 2.40 J/cm @Thickness 3.20 mm, Temperature 23.0 °C | 4.50 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
Instrumented Impact Total Energy | 14.0 J @Temperature -40.0 °C | 10.3 ft-lb @Temperature -40.0 °F |
| 24.0 J @Temperature -18.0 °C | 17.7 ft-lb @Temperature -0.400 °F |
| 30.0 J @Temperature 23.0 °C | 22.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy at Peak | 11.0 J @Temperature -40.0 °C | 8.11 ft-lb @Temperature -40.0 °F |
| 19.0 J @Temperature -18.0 °C | 14.0 ft-lb @Temperature -0.400 °F |
| 22.0 J @Temperature 23.0 °C | 16.2 ft-lb @Temperature 73.4 °F |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F |
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C | 199 °F |
| 101 °C | 214 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 85.0 °C | 185 °F |
| 94.0 °C | 201 °F |
UL RTI, Electrical | 60.0 °C @Thickness 1.50 mm | 140 °F @Thickness 0.0591 in |
UL RTI, Mechanical with Impact | 60.0 °C @Thickness 1.50 mm | 140 °F @Thickness 0.0591 in |
UL RTI, Mechanical without Impact | 60.0 °C @Thickness 1.50 mm | 140 °F @Thickness 0.0591 in |
Flammability, UL94 | HB @Thickness 1.47 mm | HB @Thickness 0.0579 in |
Flame Spread | 35.6 mm/min @Thickness 3.20 mm | 1.40 in/min @Thickness 0.126 in |
|
Optical Properties | Metric | English | Comments |
---|
Gloss | 90 % | 90 % |
|
Processing Properties | Metric | English | Comments |
---|
Rear Barrel Temperature | 215 - 240 °C | 419 - 464 °F |
Middle Barrel Temperature | 215 - 240 °C | 419 - 464 °F |
Front Barrel Temperature | 215 - 240 °C | 419 - 464 °F |
Die Temperature | 210 - 240 °C | 410 - 464 °F |
Melt Temperature | 215 - 249 °C | 419 - 480 °F |
Roll Temperature | 63.0 - 85.0 °C | 145 - 185 °F |
| 71.0 - 93.0 °C | 160 - 199 °F |
| 77.0 - 99.0 °C | 171 - 210 °F |
| 82.0 - 105 °C | 180 - 221 °F |
| 82.0 - 105 °C | 180 - 221 °F |
| 82.0 - 105 °C | 180 - 221 °F |
Drying Temperature | 82.0 - 93.0 °C @Time 10800 - 14400 sec | 180 - 199 °F @Time 3.00 - 4.00 hour |
Moisture Content | <= 0.030 % | <= 0.030 % |
Dew Point | <= -29.0 °C | <= -20.2 °F |
|
Descriptive Properties |
---|
Pump Ratio | 1.5-2.0 |
Screw Compression Ratio | 2.5-2.7 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.