MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pyrotek Pyrocast TG Castable Refractory
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Pyrocast TG is a technical-grade silica based refractory developed for the non-ferrous industry including nickel, copper, zinc, and their alloys.

Applications

  • Coreless induction furnace lining
  • Channel-type furnace lining
  • Kilns
  • Boilers
  • Heat treating furnaces
  • Forge furnaces
  • Copper base alloys

Advantages

  • Excellent thermal shock resistance
  • Dimensionally stable
  • Good insulation for density
  • Does not inhibit induction energy transfer

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.875 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00800 GPa
@Temperature 850 °C
Compressive Strength 38.0 MPa
@Temperature 850 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.250 µm/m-°C
@Temperature <=1010 °C
Thermal Conductivity 0.600 W/m-K
@Temperature 540 °C
 0.610 W/m-K
@Temperature 295 °C
 0.780 W/m-K
@Temperature 815 °C
Maximum Service Temperature, Air 1480 °C
Shrinkage 0.20 %
@Temperature 1090 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ceradyne Thermo-Sil® Castable TG Fused Silica
Pyrotek Pyrocast AR LITE Castable Refractory
Ceradyne Thermo-Sil® Castable 120 Fused Silica
Ceradyne Thermo-Sil® Castable 220 Fused Silica
Pyrotek Pyrocast AR-S Castable Refractory

CPYRO142 / 1863

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.