A light weight highly insulating refractory product which offers excellent resistance to molten aluminum erosion and thermal shock. Applications - For conveyance and casting of aluminum and its alloys
Advantages - Excellent durability
- Superior insulating properties
- Pre-fired
- Low start-up shrinkage
- Dimensionally stable at working temperature
Information provided by Pyrotek. |