MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Eastman Tritan™ LX500 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Product Description: Eastman Tritan™ LX500 is an amorphous copolyester specifically developed for use in blow molding applications for the cosmetic, fragrance, and personal care markets. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. In addition, this new generation copolyester offers excellent appearance and clarity.

Application/Uses:

  • Cosmetics hot-fill packaging
  • Cosmetics/personal care packaging
  • Fragrance packaging
Key Attributes:
  • Ease of processing
  • Excellent clarity
  • Fast drying times
  • Good chemical resistance
  • Good heat resistance
  • Outstanding impact resistance
  • Quick cycle times

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccASTM D792
Linear Mold Shrinkage 0.0060 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 110ASTM D785
Tensile Strength at Break 51.0 MPaISO 527
 52.0 MPaASTM D638
Tensile Strength, Yield 45.0 MPaASTM D638
 45.0 MPaISO 527
Elongation at Break 139 %ASTM D638
 142 %ISO 527
Elongation at Yield 7.0 %ASTM D638
 7.0 %ISO 527
Tensile Modulus 1569 MPaISO 527
 1609 MPaASTM D638
Flexural Strength 60.0 MPaISO 178
Flexural Yield Strength 64.0 MPaASTM D790
Flexural Modulus 1494 MPaISO 178
 1522 MPaASTM D790
Izod Impact, Notched 842 J/mASTM D256
Izod Impact, Unnotched NBASTM D4812
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Temperature -40.0 °C
ISO 180
 78.0 kJ/m²
@Temperature 23.0 °C
ISO 180
Puncture Energy 62.0 J
@Temperature 23.0 °C
Energy @ Max. Load; ASTM D3763
 65.0 J
@Temperature 0.000 °C
Energy @ Max. Load; ASTM D3763
 67.0 J
@Temperature -40.0 °C
Energy @ Max. Load; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 101 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %ASTM D1003
Transmission, Visible 91 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 235 - 255 °CEBM Processing
 260 - 280 °CISBM Processing
Mold Temperature 15.0 - 50.0 °CEBM Blow Mold
 35.0 - 55.0 °CISBM Blow Mold
 40.0 - 65.0 °CISBM Injection
Drying Temperature 88.0 °C
Dry Time 4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Tritan™ MX731 Medical Grade Copolyester
Avient Versaflex™ OM 2262 Thermoplastic Elastomer (TPE)
Eastman Tritan™ EX501 Copolyester
Eastman Tritan™ GX100 Copolyester
Eastman Tritan™ LX100 Copolyester

PEATM5196 / 222390

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.