MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Glyptal 1209 Black Enamel
Categories: Polymer; Thermoset; Alkyd

Material Notes: GLYPTAL 1209 BLACK ENAMEL is an air drying or baking gloss interior enamel designed for its resistance properties as well as being a protective and decorating coating for electrical equipment. It is similar to GLYPTAL 1201 RED and will give very good oil resistance and good salt spray resistance as well as excellent non-tracking and arc resistance.

Suggested Uses: GLYPTAL 1209 is suggested for the finishing of electrical equipment for interior exposure. It is similar to 1201 in properties other than dielectric strength and may be used for coating small motor stators, field coils, end windings, bus bars, and switch bases. It is also suggested for the protection of surfaces from arcing.

Application: GLYPTAL 1209 may be applied by spray or dip methods. Surfaces to be painted should be clean and dry. Reduction: 1209 should be thinned to 23 to 28 seconds (#2 Zahn Cup) with 1500 thinner.

Surface Preparation: Surfaces to be painted should be dry and free from dirt, wax, grease, rust, and oil. Remove grease and oil by washing surface with mineral spirits. When painting over a previously glossed surface, reduce gloss by use of sandpaper or steel wool.

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 62 %Weight
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 1000 V/mil
Arc Resistance 75 sec
@Time 346000 sec
Air Dry; on Textolite
 
Thermal PropertiesOriginal ValueComments
Flash Point 69.0 °F
 
Processing PropertiesOriginal ValueComments
Dry Time 4.00 hour
 
Descriptive Properties
Bake Time.5-1 hr200-250°F
 1-2 hr150-200°F
ColorBlack
Coverage550 ft²/gal1 mil dried film
GlossHigh
RecoatOvernight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane, Liquid
Overview of materials for Thermoset Polyurethane, Adhesive
Overview of materials for Silicone Polyurethane, Ether Based
Glyptal 8328 Enamel
Glyptal 8001 Insulating Enamel

PGLYPT906 / 209745

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.