MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Thermal Ceramics Kaomat 200-SL Blanket
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Kaomat 2000-SL silica blanket is a high temperature "shot free" amorphous silica blanket which has been heat treated during the manufacturing process to reduce residual shrinkage. This durable product has a low thermal conductivity, high strength, and a service temperature up to 2000°F (1093°C).

Features:No “shot” blanket, Excellent dimensional stability, High tensile strength, Available in module form.

Applications:Asbestos replacement, Steam and gas turbine blanket, Insulation of marine exhaust systems, Low temperature (<1200°F {649°C}) insulation, Aluminum homogenizing furnaces, “No-shot” furnace linings.

Information provided by Thermal Ceramics

Data has not been recently verified. Please contact manufacturer for current information.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.160 - 0.176 g/cc
Thickness 6300 microns
 13000 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 18.0 - 25.0 psi
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0900 W/m-K
@Temperature 316 °C
 0.130 W/m-K
@Temperature 482 °C
 0.170 W/m-K
@Temperature 649 °C
 0.210 W/m-K
@Temperature 816 °C
Melting Point 3100 °F
Maximum Service Temperature, Air 1800 °FContinuous
 2000 °FRating
Shrinkage 0.10 - 0.30 %
@Temperature 649 °C,
Time 86400 sec
Linear
 0.20 - 0.50 %
@Temperature 816 °C,
Time 86400 sec
Linear
 0.50 - 1.0 %
@Temperature 982 °C,
Time 86400 sec
Linear
 
Component Elements PropertiesOriginal ValueComments
SiO2 >= 94 %
 
Descriptive Properties
Fiber Diameter, microns6-13
Fiber Length, cm5-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CTHERM008 / 2328

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.