MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Swamp White Oak Wood
Categories: Wood and Natural Products; Wood; Hardwood

Key Words: Quercus Bicolor; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.640 g/cc0.640 g/ccGreen, based on volume
 0.720 g/cc0.720 g/cc12% moisture content, based on volume
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 5160 N1160 lb (f)Green
 7206 N1620 lb (f)12% moisture content
Tensile Strength at Break 5.72 MPa830 psi12% moisture content, perpendicular to grain
 5.93 MPa860 psiGreen, perpendicular to grain
Modulus of Elasticity 11.0 GPa1590 ksiGreen
 14.1 GPa2050 ksi12% moisture content
Modulus of Rupture 0.0683 GPa9.90 ksiGreen
 0.122 GPa17.7 ksi12% moisture content
Compressive Strength 5.24 MPa760 psiGreen, perpendicular to grain
 8.20 MPa1190 psi12% moisture content, perpendicular to grain
 30.1 MPa4360 psiGreen, parallel to grain
 59.3 MPa8600 psi12% moisture content, parallel to grain
Shear Strength 8.96 MPa1300 psiGreen, parallel to grain
 13.8 MPa2000 psi12% moisture content, parallel to grain
Impact 4949Impact bending in inches, 12% moisture content
 5050Impact bending in inches, green
Work to Maximum Load 0.100 J/cm³14.5 in-lb/in³Green
 0.132 J/cm³19.2 in-lb/in³12% moisture content

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Red Oak Wood
Southern Magnolia Wood
Southern Red Oak Wood
American White Oak Wood
Black Ironwood Wood

PTSU044 / 71486

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.