MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil EXACT™ 3139 Plastomer for Cast Film Applications
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE

Material Notes: Product Description: Exact 3139 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3139 is designed for both monolayer and multilayer coextruded cast film applicatiosn requiring excellent toughness and heat seal performance. Typical applications include food packaging seal layers and lamination films.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Cast Film
  • Lamination Film
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ExxonMobil Method
Thickness 25.4 microns1.00 mil
Melt Flow 7.5 g/10 min7.5 g/10 minExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 5.24 MPa760 psiASTM D882
Film Tensile Strength at Yield, TD 4.48 MPa650 psiASTM D882
Film Elongation at Break, MD 530 %530 %ASTM D882
Film Elongation at Break, TD 700 %700 %ASTM D882
Film Elongation at Yield, MD 10.2 %10.2 %ASTM D882
Film Elongation at Yield, TD 8.1 %8.1 %ASTM D882
Puncture Energy 5.29 J3.90 ft-lbExxonMobil Method
Elmendorf Tear Strength, MD 13.8 g/micron350 g/milASTM D1922
Elmendorf Tear Strength, TD 25.2 g/micron640 g/milASTM D1922
Dart Drop 9.45 g/micron240 g/milASTM D1709A
Film Tensile Strength at Break, MD 65.8 MPa9540 psiASTM D882
Film Tensile Strength at Break, TD 55.6 MPa8060 psiASTM D882
1% Secant Modulus, MD 67.6 MPa9800 psiASTM D882
1% Secant Modulus, TD 75.8 MPa11000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 94.4 °C202 °FPeak Melting Temperature; ExxonMobil Method
Crystallization Temperature 78.0 °C172 °FExxonMobil Method
Vicat Softening Point 80.0 °C176 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 0.50 %0.50 %ASTM D1003
Gloss 92 %92 %ASTM D2457
 
Descriptive Properties
Puncture Force11 lbfExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil EXACT™ 8210 Plastomer for Multilayer Film Applications
ExxonMobil LLDPE LL 1001X31 Linear Low Density Polyethylene Resin
ExxonMobil LL 3003.32 Cast Film Resin
ExxonMobil LL 1002x75 Blown Film Resin

PEXB349 / 37654

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.