Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular material which, while it can be used for film production, is also suitable for compounding. Availability: Latin America, North America and South America Additive: - Antiblock: 7500 ppm
- Slip: 1350 ppm
- Processing Aid: No
- Thermal Stabilizer: Yes
Applications: - Agricultural Film
- Bag in Box
- Blown Film
- Cast Film
- Food packaging
- Form Fill and Seal Packaging
- Freezer Film
- Garment Film
- General Packaging
- Industrial Packaging
- Liners
- Mulch Film
- Packaging Films
- Produce Bags on a Roll
- Shoppers
- Trash Can Liners
Information provided by ExxonMobil Chemical |