MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Henkel Loctite® ABLESTIK 84-1LMISR4 Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Appearance: Silver

Product Benefits:

  • Conductive
  • Box oven cure
  • Excellent dispensability, minimal tailing and stringing
Cure: Heat cure

Application: Die attach

LOCTITE ABLESTIK 84-1LMISR4 electrically conductive die attach adhesive has been formulated for use in high throughput, automated die attach equipment. The rheology of LOCTITE ABLESTIK 84-1LMISR4 adhesive allows minimum adhesive dispense and die put down dwell times, without tailing or stringing problems. The unique combination of adhesive properties makes this material one of the most widely used die attach materials in the semiconductor industry.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Moisture Absorption 0.600 %
@Temperature 85.0 °C
0.600 %
@Temperature 185 °F
Cured @ Saturation, after 85% RH exposure
pH 6.06.0
Brookfield Viscosity 8000 cP8000 cPUncured, CP51, Speed 10 rpm
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus  0.300 GPa
@Temperature 250 °C
43.5 ksi
@Temperature 482 °F
Cured
 2.00 GPa
@Temperature 150 °C
290 ksi
@Temperature 302 °F
Cured
 3.90 GPa
@Temperature 25.0 °C
566 ksi
@Temperature 77.0 °F
Cured
 4.40 GPa
@Temperature -65.0 °C
638 ksi
@Temperature -85.0 °F
Cured
Shear Strength 7.00 MPa1020 psiLap
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.00020 ohm-cm<= 0.00020 ohm-cmCured
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C22.2 µin/in-°FCured, Below Tg
 150 µm/m-°C83.3 µin/in-°FCured, Above Tg
Thermal Conductivity 2.50 W/m-K
@Temperature 121 °C
17.4 BTU-in/hr-ft²-°F
@Temperature 250 °F
Cured
Glass Transition Temp, Tg 120 °C248 °FCured, TMA
 
Processing PropertiesMetricEnglishComments
Cure Time 3.00 - 5.00 min0.0500 - 0.0833 hourminute ramp to 175°C + 1 hour @ 175°C, Alternate Cure Schedule
 60.0 min
@Temperature 175 °C
1.00 hour
@Temperature 347 °F
Working Life 1080 min1080 min
Shelf Life 12.0 Month
@Temperature 5.00 °C
12.0 Month
@Temperature 41.0 °F
Uncured, from date of manufacture
 
Descriptive Properties
Extractable Ionic Content (ppm)<10Cured, Sodium (Na+)
 <10Cured, Potassium (K+)
 <20Cured, Chloride (Cl-)
Shear Strength>2.8 kg@ 150°C, 2 X 2 mm (80 x 80 mil) Si die on Ag/Cu LF
 >8 kg@ 25°C, 2 X 2 mm (80 x 80 mil) Si die on Ag/Cu LF
 1.4 kg-f/dieOn Bare Cu LF @ 250°C, Post Cure, 3 X 3 mm (120 x 120 mil) Si die
 1.7 kg-f/dieOn Ag/Cu LF @ 250°C, Post Cure, 3 X 3 mm (120 x 120 mil) Si die
 1.8 kg-f/dieOn Ag/Cu LF @ 200°C, After 85ºC/85% RH exposure for 168 hours
 1.8 kg-f/dieOn Pd/Ni/Cu LF @ 200°C, After 85ºC/85% RH exposure for 168 hours
 10 kg-f/dieOn Bare Cu LF @ 25°C, After 85ºC/85% RH exposure for 168 hours
 11 kg-f/dieOn Bare Cu LF @ 25°C, Post Cure, 3 X 3 mm (120 x 120 mil) Si die
 12 kg-f/dieOn Ag/Cu LF @ 25°C, After 85ºC/85% RH exposure for 168 hours
 2 kg-f/dieOn Pd/Ni/Cu LF @ 250°C, Post Cure, 3 X 3 mm (120 x 120 mil) Si die
 2.4 kg-f/dieOn Pd/Ni/Cu LF @ 200°C, Post Cure, 3 X 3 mm (120 x 120 mil) Si die
 2.5 kg-f/dieOn Bare Cu LF @ 200°C, After 85ºC/85% RH exposure for 168 hours
 2.6 kg-f/dieOn Bare Cu LF @ 200°C, Post Cure, 3 X 3 mm (120 x 120 mil) Si die
 2.9 kg-f/dieOn Ag/Cu LF @ 200°C, Post Cure, 3 X 3 mm (120 x 120 mil) Si die
 21 kg-f/dieOn Ag/Cu LF @ 25°C, Post Cure, 3 X 3 mm (120 x 120 mil) Si die
 23 kg-f/dieOn Pd/Ni/Cu LF @ 25°C, After 85ºC/85% RH exposure for 168 hours
 27 kg-f/dieOn Pd/Ni/Cu LF @ 25°C, Post Cure, 3 X 3 mm (120 x 120 mil) Si die
Thixotropic Index5.6Uncured, 0.5/5 rpm
Water Extract Conductivity<2 µmhos/cmCured
Weight Loss (%)0.35Cured @ 300ºC, TGA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLOCT5005 / 255216

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.