MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Applications
Alathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications include housewares, containers, caps and closures.

Regulatory Status
H5220 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520.

Processing Techniques
Specific recommendations for processing H5220 can only be made when the processing conditions, equipment and end-use applications are known.

Key Words: FDA 21 CFR 177.1520.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 33.0 - 37.0 lb/ft³ASTM D1895
Density 0.952 g/ccASTM D1505
Melt Flow 20 g/10 min
@Load 0.980 kg,
Temperature 190 °C
ASTM D1238
Spiral Flow 11.6 inEquistar
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 76ASTM D2240
Tensile Strength, Yield 3790 psi50 mm/min, Type IV; ASTM D4796
Elongation at Yield 11 %50 mm/min, Type IV; ASTM D638
Tensile Modulus 145000 psi1% Secant, 50mm/min; ASTM D638
 183000 psi50 mm/min; ASTM D638
Flexural Modulus 181000 psiASTM D790
Flexural Modulus, 1% Secant 157000 psi12.5mm/min; ASTM D790
2% Secant Modulus 131000 psi12.5mm/min; ASTM D790
Izod Impact, Notched 0.710 ft-lb/in
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched NB
@Temperature -18.0 °C
ASTM D4812
 
Thermal PropertiesOriginal ValueComments
Melting Point 266.4 °FASTM D3418
Crystallization Temperature 239.7 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 163 °FASTM D648
Vicat Softening Point 256 °FASTM D1525
Brittleness Temperature <= -105 °FF50; ASTM D746
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 450 °F
Middle Barrel Temperature 470 °F
Front Barrel Temperature 475 °F
Nozzle Temperature 475 °F
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total 6280 High Density Polyethylene, Injection Molding Resin
Bamberger Polymers Bapolene® 3262 Polyethylene, Injection Grade
Dow UNIVAL™ DMDC-6143 NT 7 High Density Polyethylene Resin (HDPE)
Bamberger Polymers Bapolene® 3257U Polyethylene, Injection Molding
Global V-1160 High Density Polyethylene, Injection Molding Grade

PEQU0850 / 157471

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.