MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Applications
Alathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications include housewares, containers, caps and closures.

Regulatory Status
H5220 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520.

Processing Techniques
Specific recommendations for processing H5220 can only be made when the processing conditions, equipment and end-use applications are known.

Key Words: FDA 21 CFR 177.1520.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.529 - 0.593 g/cc0.0191 - 0.0214 lb/in³ASTM D1895
Density 0.952 g/cc0.0344 lb/in³ASTM D1505
Melt Flow 20 g/10 min
@Load 0.980 kg,
Temperature 190 °C
20 g/10 min
@Load 2.16 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow 29.5 cm11.6 inEquistar
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7676ASTM D2240
Tensile Strength, Yield 26.1 MPa3790 psi50 mm/min, Type IV; ASTM D4796
Elongation at Yield 11 %11 %50 mm/min, Type IV; ASTM D638
Tensile Modulus 1.00 GPa145 ksi1% Secant, 50mm/min; ASTM D638
 1.26 GPa183 ksi50 mm/min; ASTM D638
Flexural Modulus 1.25 GPa181 ksiASTM D790
Flexural Modulus, 1% Secant 1080 MPa157000 psi12.5mm/min; ASTM D790
2% Secant Modulus 0.903 GPa131 ksi12.5mm/min; ASTM D790
Izod Impact, Notched 0.379 J/cm
@Temperature 23.0 °C
0.710 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB
@Temperature -18.0 °C
NB
@Temperature -0.400 °F
ASTM D4812
 
Thermal PropertiesMetricEnglishComments
Melting Point 130.2 °C266.4 °FASTM D3418
Crystallization Temperature 115.4 °C239.7 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 72.8 °C163 °FASTM D648
Vicat Softening Point 124 °C256 °FASTM D1525
Brittleness Temperature <= -76.1 °C<= -105 °FF50; ASTM D746
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 232 °C450 °F
Middle Barrel Temperature 243 °C470 °F
Front Barrel Temperature 246 °C475 °F
Nozzle Temperature 246 °C475 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total 6280 High Density Polyethylene, Injection Molding Resin
Bamberger Polymers Bapolene® 3262 Polyethylene, Injection Grade
Dow UNIVAL™ DMDC-6143 NT 7 High Density Polyethylene Resin (HDPE)
Bamberger Polymers Bapolene® 3257U Polyethylene, Injection Molding
Global V-1160 High Density Polyethylene, Injection Molding Grade

PEQU0850 / 157471

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.