MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem HM 150 HDPE Monofilament Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes:

Applications: Raschel; flat yarn; general and industrial rape netting.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D1505
ESCR 100% Igepal® 24 hour
@Thickness 3.00 mm,
Temperature 23.0 °C
24 hour
@Thickness 0.118 in,
Temperature 73.4 °F
compression molded plaques; ASTM D1693B
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464ASTM D2240
Tensile Strength at Break 33.0 MPa4790 psiASTM D638
Film Tensile Strength at Yield, MD 26.0 MPa3770 psiASTM D882
Film Tensile Strength at Yield, TD 30.0 MPa4350 psiASTM D882
Tensile Strength, Yield 28.0 MPa4060 psiASTM D638
Film Elongation at Break, MD 1300 %1300 %ASTM D882
Film Elongation at Break, TD >= 1700 %>= 1700 %ASTM D882
Flexural Modulus 1.145 GPa166.1 ksiASTM D790
Elmendorf Tear Strength, MD 0.700 g/micron17.8 g/milASTM D1922
Elmendorf Tear Strength, TD 1.90 g/micron48.3 g/milASTM D1922
Film Tensile Strength at Break, MD 49.0 MPa7110 psiASTM D882
Film Tensile Strength at Break, TD 48.0 MPa6960 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 126 °C259 °FASTM D1525
 
Descriptive Properties
Minimum Recommended Thickness15 µm
Puncture Strength26 J/mmBraskem® Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem Green PE SHA7260 Injection Molding High Density Polyethylene
LyondellBasell Alathon® L5045 High Density Polyethylene
Borealis BorPure™ MB7541 High Density Polyethylene for Injection Molding
Borealis Borstar® CB9600 HDPE for Extrusion Coating
Borealis Borstar® MB7542 High Density Polyethylene for Injection Molding

PBRAS074 / 27808

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.