MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis BorPure™ MB7541 High Density Polyethylene for Injection Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: MB7541 is a bimodal, natural, high density polyethylene produced by the Borstar PE technology. MB7541 combines excellent organoleptic properties, Environmental Stress Crack Resistance (ESCR) and superior flow properties as well as good impact strength and toughness even at low temperatures. The improved processability, also at low melt temperature, allows energy savings and faster cycle time. MB7541 is designed for injection and compression molding.

MB7541 is recommended for products requiring good environmental stress crack resistance and/or organoleptic properties and impact strength.

Former trade name for this product was Borstar®.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.954 g/cc0.0345 lb/in³ISO 1183
ESCR 10% Igepal® >= 40 hour>= 40 hourASTM D1693
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6161ISO 868
Tensile Strength, Yield 22.0 MPa3190 psiAt 50 mm/min; ISO 527-2
Elongation at Yield 10 %10 %At 50 mm/min; ISO 527-2
Tensile Modulus 0.850 GPa123 ksiAt 1 mm/min; ISO 527-2
Tensile Impact Strength 80.0 kJ/m²38.1 ft-lb/in²At 23°C; ISO 8256/A1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 250 °C374 - 482 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Borstar® MB7542 High Density Polyethylene for Injection Molding
Braskem HC7260LS-L HDPE Injection Molding Polyethylene
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Braskem HD7255LS-L HDPE Injection Molding Polyethylene
Borealis BL0521 High Density Polyethylene

PBOREA131 / 27438

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.