MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
E-Polymers Tekaloy® G70FR , Flame Retardant, Un-Reinforced PC/ABS Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Flame Retardant, Impact Resistance

Information provided by E-Polymers Co. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
Melt Flow 6.2 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 114ASTM D785
Tensile Strength, Yield 57.0 MPaASTM D638
Elongation at Break 50 %ASTM D638
Flexural Yield Strength 8.20 MPaASTM D790
Flexural Modulus 2.30 GPaASTM D790
Izod Impact, Notched 6.10 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 111 °CASTM D648
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Processing Temperature 210 - 260 °C
Mold Temperature 60.0 - 90.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chi Mei Wonderloy® PC-540 PC/ABS Alloy - Flame Retardant
A. Schulman Diamond DIAMALOY 750 ABS/PC Alloy, Non-Halogen, Flame Retardant
Covestro Bayblend® T80 XG PC/ABS Blend
E-Polymers Tekaloy® G70GFR , Flame Retardant, 30% Glass Fiber Reinforced PC/ABS Alloy
E-Polymers TEKALOY® G70NHT Non Halogen Flame Retardant Impact Resistance PC/ABS Alloy

PEPOLY46 / 36348

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.