MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman Diamond DIAMALOY 750 ABS/PC Alloy, Non-Halogen, Flame Retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes:

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Engineered Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/inASTM D955
Melt Flow  3.9 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.9 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 11.8 g/10 min
@Load 3.80 kg,
Temperature 230 °C
11.8 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 61.5 MPa8920 psichs 2.0 in/min; ASTM D638
Elongation at Yield 4.5 %4.5 %chs 2.0 in/min; ASTM D638
Flexural Modulus 2.584 GPa374.8 ksichs 0.05 in/min; ASTM D790
Izod Impact, Notched 7.48 J/cm
@Thickness 3.17 mm
14.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 113 °C
@Load 1.00 kg,
Thickness 3.17 mm
235 °F
@Load 2.20 lb,
Thickness 0.125 in
ASTM D1527
Flammability, UL94  V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
 5VB
@Thickness 20.1 mm
5VB
@Thickness 0.790 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Diamond DIAMALOY 761 ABS/PC Alloy, Non-Halogen Flame Retardant with 5% PTFE
A. Schulman Diamond DIAMALOY 750 HF PLATABLE ABS/PC Alloy, Platable Non-Halogen, Flame Retardant
A. Schulman Diamond DIAMALOY ABSPC 750 HF ABS/PC Alloy, Non-Halogen, Flame Retardant
A. Schulman Diamond DIAMALOY 730 ABS/PC Alloy, Flame Retardant
BASF Elastollan® 1154 D FHF TPUR Flame Retardant Halogen Free

PDIAM382 / 126473

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.