Developmental Product Description: Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength makes DA528 an excellent choice for profile extrusions, molding, and foaming applications requiring high VA content. Application/Uses:- Flexible packaging films
- Peelable seals, adhesive layers
- Injection and blow molding
- Hot melt adhesives and blends
- Profile extrusions, tubing, wire & cable
Information provided by Westlake Chemical |