MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Westlake Elevate™ DA528AA Ethylene Vinyl Acetate Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Developmental Product

Description: Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength makes DA528 an excellent choice for profile extrusions, molding, and foaming applications requiring high VA content.

    Application/Uses:
  • Flexible packaging films
  • Peelable seals, adhesive layers
  • Injection and blow molding
  • Hot melt adhesives and blends
  • Profile extrusions, tubing, wire & cable

Information provided by Westlake Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D1505
Melt Flow 2.5 g/10 min2.5 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Dart Drop Test 390 g0.860 lbASTM D1709
Film Tensile Strength at Break, MD 24.8 MPa3600 psiASTM D882
Film Tensile Strength at Break, TD 24.1 MPa3500 psiASTM D882
1% Secant Modulus, MD 42.1 MPa6100 psiASTM D882
1% Secant Modulus, TD 50.3 MPa7300 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 85.0 °C185 °FPeak, by DSC; ASTM D3418
Flash Point >= 343 °C>= 649 °FASTM E136
 
Optical PropertiesMetricEnglishComments
Haze 3.5 %3.5 %ASTM D1003
Gloss 82 %82 %@ 45°; ASTM D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical SEETEC ES440 Ethylene Vinyl Acetate
LG Chemical SEETEC EF443 Ethylene Vinyl Acetate
LG Chemical SEETEC EF321 Ethylene Vinyl Acetate
LG Chemical SEETEC EF320 Ethylene Vinyl Acetate
LG Chemical SEETEC EF221 Ethylene Vinyl Acetate

PWESF8918 / 133463

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.