MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218 V40 Black 21 N PA 66 40% Glass Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Description: TECHNYL® A 218 V40 Black 21 N is a polyamide 66, reinforced with 40% of glass fiber, heat stabilized, for injection molding. This product is available in black color.

Key Properties: Mechanical performance; Heat stabilized

Benefits: The product offers an excellent combination between thermal and mechanical properties.

Applications: It is used in a wide variety of industries.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccISO 1183/A
Water Absorption 0.70 %
@Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0057 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0040 cm/cm
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 225 MPaISO 527 Type 1A
Elongation at Break 2.0 %ISO 527 Type 1A
Tensile Modulus 13000 MPaISO 527 Type 1A
Flexural Modulus 10800 MPaISO 178
Izod Impact, Notched (ISO) 13.5 kJ/m²ISO 180/1A
Charpy Impact Unnotched 97.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 6.00e+14 ohmIEC 60093
Dielectric Constant 3.7IEC 60250
Dielectric Strength 35.0 kV/mmIEC 60243
Dissipation Factor 0.010IEC 60250
Comparative Tracking Index 450 VSol A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 263 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 255 °CISO 75/Af
Flammability, UL94 HB
@Thickness 1.60 mm
ISO 1210
Oxygen Index 23 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 280 °CCompression zone
 280 - 290 °CMixing zone
Feed Temperature 260 - 270 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® 70G30L NC010 PA66-GF30
Celanese Zytel® 70G43HSLA BK099 PA66-GF43
Domo TECHNYL® A 218 V40 Black 21 N PA 66 40% Glass Reinforced, Conditioned
Celanese Zytel® 70G50HSLA BK039B PA66-GF50
Celanese Zytel® 70G35HSL NC010 PA66-GF35

PSOLVAY834 / 218562

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.