MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.

Data provided by BP Amoco; Curv was spun off from BP Amoco in 2004 and is now a product of Propex Fabrics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccASTM D792
 0.920 g/ccISO 1183
Water Absorption <= 0.10 %DIN 53495
 <= 0.10 %20°C; ASTM D570-81
 <= 0.10 %100°C; ASTM D570-81
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 35.0 MPaEN ISO 2039-1
Tensile Strength, Ultimate 120 MPaMD; DIN EN ISO 527
 120 MPaCD; DIN EN ISO 527
 180 MPaASTM D638M-92
Elongation at Break 16.6 %ASTM D638M-92
 20 %MD; DIN EN ISO 527
 20 %CD; DIN EN ISO 527
Tensile Modulus 4.20 GPaMD; DIN EN ISO 527
 4.20 GPaCD; DIN EN ISO 527
 5.00 GPaASTM D638M-93
Flexural Strength 80.0 MPaMD; DIN EN ISO 178
 80.0 MPaCD; DIN EN ISO 178
 107.7 MPaASTM D790M-93
Flexural Modulus 3.50 GPaMD; DIN EN ISO 178
 3.50 GPaCD; DIN EN ISO 178
 3.60 GPaASTM D790M-93
Compressive Strength >= 300 MPaNormal to Plane; EN ISO 604
Izod Impact, Notched 47.5 J/cmASTM D256-93a
 75.0 J/cm
@Temperature -40.0 °C
ASTM D256-93a
Izod Impact, Notched (ISO) 400 kJ/m²22 J; EN ISO 180/2 ep b
 600 kJ/m²
@Temperature -40.0 °C
22 J; EN ISO 180/2 ep b
Izod Impact, Unnotched (ISO) NB22 J; EN ISO 180/2 ep
Charpy Impact Unnotched NBEN ISO 179/2 ep
 NBLow Temp; EN ISO 179/2 ep
Charpy Impact, Notched 12.0 J/cm²EN ISO 179/2 ep b
Tensile Impact Strength 1000 kJ/m²MD; EN ISO 8256
 1000 kJ/m²CD; EN ISO 8256
Puncture Energy 17.6 J70°C High Speed Puncture Energy; ASTM D3763-97a
 21.6 J100°C High Speed Puncture Energy; ASTM D3763-97a
 40.0 JPuncture Impact; 52 J; 2.1 mm; ISO 6603
 14.1 J
@Temperature -40.0 °C
High Speed Puncture Energy; ASTM D3763-97a
Torsional Stiffness 1200 MPaDIN EN ISO 6721
 
Thermal PropertiesOriginal ValueComments
CTE, linear 41.0 µm/m-°C
@Temperature 20.0 °C
Temp range not reported; ASTM D696
 68.0 µm/m-°C
@Temperature 20.0 - 80.0 °C
DIN 53752
Deflection Temperature at 0.46 MPa (66 psi) 160 °Cflatwise; EN ISO 75-2B
 160 °CASTM D648-82/88
Deflection Temperature at 1.8 MPa (264 psi) 102 °CASTM D648-82/88
 102 °Cflatwise; EN ISO 75-2A
Vicat Softening Point 175 °C50K/h; DIN EN ISO 306
 
Descriptive Properties
Fire Behavior of Building MaterialsPassed B 2DIN 4102

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Sheet/Thermoforming Grade
SEKISUI SPI KYDEX® T Thermoplastic
DuPont Mobility and Materials Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA) (Extended Tabular Temperature Data)
Ensinger TECASINT 1011 Polyimide (PI)
LATI Latamid 6 H2E04 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized

PBPCURV / 27640

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.