MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion AlBeMet® AM 162 Rolled Sheet, Annealed
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Beryllium Alloy

Material Notes: Mechanical properties are typical, longitudinal values at RT. AlBeMet® AM 162 is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are derived by consolidating the Al/Be powder by hot isostatic pressing (HIP) and cold isostatic pressing (CIP) followed by extrusion or sheet rolling processes.

Used for heat sinks and structural parts in aircraft and satellite avionics because of its low density, high modulus, high thermal conductivity, low CTE, and thermal stability.

Please note that there are health hazards associated with beryllium, especially when present as airborne particles generated during processing. As with any material, be aware of hazards and take steps to reduce exposure to a safe level.

Information provided by Brush Wellman.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Key Words: Aluminum Beryllium Composite Alloy AM162
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.071 g/cc0.07482 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 6868
Tensile Strength, Ultimate >= 379 MPa>= 55000 psi
 435 MPa63100 psiTypical
Tensile Strength, Yield >= 276 MPa>= 40000 psi
 321 MPa46600 psiTypical
Elongation at Break >= 5.0 %>= 5.0 %
 9.0 %9.0 %Typical
Modulus of Elasticity 193 GPa28000 ksi
Poissons Ratio 0.170.17
Shear Modulus 82.0 GPa11900 ksicalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000350 ohm-cm
@Temperature 20.0 °C
0.00000350 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.91 µm/m-°C
@Temperature 25.0 °C
7.728 µin/in-°F
@Temperature 77.0 °F
Specific Heat Capacity 1.56 J/g-°C
@Temperature 20.0 °C
0.373 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 210 W/m-K1460 BTU-in/hr-ft²-°F
Melting Point 644 - 1082 °C1190 - 1980 °F
Solidus 644 °C1190 °F
Liquidus 1082 °C1980 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 35 - 40 %35 - 40 %As remainder
Beryllium, Be 60 - 64 %60 - 64 %
Carbon, C <= 0.10 %<= 0.10 %
Other, each <= 0.20 %<= 0.20 %
Oxygen, O <= 1.0 %<= 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion AlBeMet® AM 162 Extruded Bar, Annealed
Materion AlBeMet® AM 162 HIP'd Billet, Annealed
Materion AlBeCast™ IC910 Aluminum Beryllium Composite
Goodfellow Aluminum-Lithium/SiC Metal Matrix Composite
Aluminum - SiC Metal Matrix Composite

NBB002 / 15088

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.