MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion AlBeCast™ IC910 Aluminum Beryllium Composite  (discontinued **)
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Beryllium Alloy

Material Notes: Mechanical properties are typical values at RT. AlBeCast™ IC910 is an aluminum-beryllium alloy that combines the advantages of a net shape casting technology, investment casting, with the stiffness, thermal performance, and weight savings of Al/Be materials. The casting process requires little change from Al or Ti casting.

Please note that there are health hazards associated with beryllium, especially when present as airborne particles generated during processing. As with any material, be aware of hazards and take steps to reduce exposure to a safe level.

Information provided by Brush Wellman.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.17 g/cc0.0784 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 207 MPa30000 psi
Tensile Strength, Yield 158 MPa
@Strain 0.2 %
22900 psi
@Strain 0.2 %
Elongation at Break 4.0 %4.0 %
Tensile Modulus 192 GPa27800 ksiDynamic modulus
 193 GPa28000 ksi
Compressive Yield Strength 147 MPa21300 psi
Poissons Ratio 0.1540.154
Fatigue Strength 117 MPa
@# of Cycles 1.00e+7
17000 psi
@# of Cycles 1.00e+7
R=0.05; Kt = 2.16 MPa
Fracture Toughness 7.30 - 14.6 MPa-m½6.64 - 13.3 ksi-in½KQ
Shear Modulus 84.0 GPa12200 ksidynamic
Shear Strength 181 MPa26300 psidouble pin shear (ASTM B-789)
 
Thermal PropertiesMetricEnglishComments
CTE, linear  14.6 µm/m-°C
@Temperature 20.0 °C
8.11 µin/in-°F
@Temperature 68.0 °F
 16.0 µm/m-°C
@Temperature 250 °C
8.89 µin/in-°F
@Temperature 482 °F
 18.2 µm/m-°C
@Temperature 500 °C
10.1 µin/in-°F
@Temperature 932 °F
Specific Heat Capacity 1.56 J/g-°C0.373 BTU/lb-°F
Thermal Conductivity 110 W/m-K763 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 38 %38 %As remainder
Beryllium, Be 57 - 63 %57 - 63 %
Iron, Fe <= 0.30 %<= 0.30 %
Nickel, Ni 2.1 - 3.4 %2.1 - 3.4 %
Oxygen, O <= 0.24 %<= 0.24 %
Silicon, Si <= 0.50 %<= 0.50 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion AlBeMet® AM 162 Extruded Bar, Annealed
Materion AlBeMet® AM 162 Rolled Sheet, Annealed
Materion AlBeMet® AM 162 HIP'd Billet, Annealed
Goodfellow Aluminum-Lithium/SiC Metal Matrix Composite
Aluminum - SiC Metal Matrix Composite

NBB100 / 15089

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.