MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Skybond® 800 Aromatic Polyimide Two Stage Resin
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: Two-stage cure polyimide resin that when used in prepreg applications allows the manufacture of very low void level composites by autoclave processing (<0.5% voids), combined with excellent thermal stability.

Information provided by Industrial Summit Technology Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 41 - 43 %41 - 43 %
Viscosity 500 - 2000 cP
@Temperature 250 °C
500 - 2000 cP
@Temperature 482 °F
Melt
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 295 - 305 °C563 - 581 °FResin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger XP-131 Compression Molded Unfilled PI
Ensinger TECASINT™ 2021 Polyimide, Brown (PI)
Ensinger TECASINT 3062 Polyimide, Shiny Black, 15% Graphite, 10% PTFE (PI)
Ensinger TECASINT 3012 Polyimide, Ochre Brown (PI)
Ensinger Sintimid™ V 15% graphite Polyimide (PI)

PISTEC990 / 183052

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.