MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil HD 5530HL High Density Polyethylene (HDPE), Copolymer Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Copolymer Film Grade

Material Notes: ExxonMobil™ HD 5530HL is a high molecular weight, high-density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity

Availability:  Africa & Middle East, Europe, Latin America, North America

Applications: drums, heavy gauge sheet, thermoformed parts, food packaging, large part blow molding, highway drainage pipe, shot gun shells.  Forms:  pellets.  Processing Method:  blow molding, sheet extrusion, thermoforming.

Information provided by ExxonMobil.

Key Words: Paxon™ BA54-030
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.956 g/ccASTM D4883
ESCR 100% Igepal® 580 hourASTM D1693
Melt Flow <= 0.10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
High Load Melt Index 2.8 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4000 psiASTM D638
Flexural Modulus 120000 psiASTM D790
Flexural Modulus, 1% Secant 570000 psi1.3 mm/min; ASTM D790
Charpy Impact, Notched 4.50 J/cm²
@Temperature -20.0 °C
ISO 179/1eA
 6.10 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 133 °C
Crystallization Temperature 118 °C
Vicat Softening Point 264 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Paxon™ HYA021L High Density Polyethylene (HDPE), Copolymer Film Grade
ExxonMobil HDP 8760.29 High Density Polyethylene (HDPE), Copolymer Film Grade
ExxonMobil HDP 8660.29 High Density Polyethylene (HDPE), Copolymer Film Grade
ExxonMobil HD 6001 High Density Polyethylene (HDPE), Film Grade
Dow HDPE 65053N High Density Polyethylene

PEX98890 / 238272

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.