MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SEKISUI SPI ALLEN® 8300FR PC/ABS Sheet
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: ALLEN® 8300FR is a polycarbonate and ABS blend with high impact properties, stiffness, heat resistance, and a non-halogenated flame retardant V-0 @ 0.060”, 5VA @ 0.118” rating.

ALLEN® 8300FR has been tested under laboratory conditions and has achieved a UL94 V-0 rating at 0.060 in (1.52mm) and above and meets the requirements of Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302).

Suggested Application:

  • Medical Equipment Housings
  • Electrical Housings and Covers
  • Vehicle Interior Trim Parts
  • Battery Charging Station
Features:
  • Flame retardant
  • Halogen free
  • Low smoke toxicity
  • High heat deflection temperature
  • Increased stiffness
  • Edge trim easily used into future orders
  • High gloss finish

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Water Absorption 0.140 %
@Time 86400 sec
0.140 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 119119ASTM D785
Tensile Strength 65.1 MPa9440 psiASTM D638
Tensile Modulus 2.63 GPa381 ksiASTM D638
Flexural Strength 100.7 MPa
@Strain 5.00 %
14610 psi
@Strain 5.00 %
ASTM D790
Flexural Modulus 2.63 GPa381 ksiASTM D790
Compressive Yield Strength 80.7 MPa11700 psiASTM D695
Bearing Yield Strength <= 293 MPa<= 42500 psiASTM D953
 29.5 MPa
@Strain 4.00 %
4280 psi
@Strain 4.00 %
ASTM D953
Shear Strength 61.9 MPa8980 psiASTM D732
Izod Impact, Notched 6.408 J/cm12.00 ft-lb/inASTM D256
Gardner Impact 68.4 J50.4 ft-lbDrop Dart Impact, GE; ASTM D5420
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 16.7 kV/mm424 kV/inoil; ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 68.0 µm/m-°C37.8 µin/in-°FASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 112 °C234 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 109 °C228 °Fannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.52 mm
V-0
@Thickness 0.0598 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSEKIS523 / 325263

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.