MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Leaded Nickel Bronze, UNS C97800, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Investment, Permanent Mold, and Sand.

Applications: Ornamental and sanitary castings, valves and valve seats, musical instrument components.

Classified under: Nickel silvers. ASTM B584; formerly ASTM B149-11B

Typical data for sand-cast test bars. Alloy does not respond to heat treating. Casting shrinkage allowance is 1.6%

Key Words: Leaded nickel silver, ASTM B584, ASTM B149-11B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.86 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 1303000 kg
Tensile Strength, Ultimate 380 MPa
Tensile Strength, Yield 205 MPa
@Strain 0.5 %
Elongation at Break 15 %in 50 mm
Modulus of Elasticity 130 GPa
Machinability 60 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00003831 ohm-cm
@Temperature 20.0 °C
4.5% IACS, as-cast tempers
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.5 µm/m-°C
@Temperature 20.0 - 260 °C
Specific Heat Capacity 0.375 J/g-°C
Thermal Conductivity 25.4 W/m-K
@Temperature 20.0 °C
Melting Point 1140 - 1180 °C
Solidus 1140 °C
Liquidus 1180 °C
Shrinkage 1.6 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 260 °CStress-Relieving Temperature
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0050 %
Antimony, Sb <= 0.20 %
Copper, Cu 64 - 67 %
Iron, Fe <= 1.5 %
Lead, Pb 1.0 - 2.5 %
Manganese, Mn <= 1.0 %
Nickel, Ni 24 - 27 %
Phosphorus, P <= 0.050 %
Silicon, Si <= 0.15 %
Sulfur, S <= 0.080 %
Tin, Sn 4.0 - 5.5 %
Zinc, Zn 1.0 - 4.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Leaded Phosphor Bronze, UNS C94400, Copper Casting Alloy
High-Leaded Tin Bronze, UNS C93900, Copper Casting Alloy
Leaded Nickel Bronze, UNS C97600, Copper Casting Alloy
Copper, UNS C62400 (Aluminum Bronze 11%)
Cast Stainless Steel CF8M, ASTM A351

MC97800b1 / 11978

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.