MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Leaded Nickel Bronze, UNS C97600, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Investment, and Sand.

Applications: Marine castings, sanitary fittings, ornamental hardware, valves, pumps.

Classified under: Nickel silvers. ASTM B584; formerly ASTM B149-11A

Data typical for sand-cast test bars. Alloy does not respond to heat treating. Casting shrinkage allowance is 2%

Key Words: Leaded nickel silver, ASTM B584, ASTM B149-11A
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.90 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 8080500 kg
Tensile Strength, Ultimate 310 MPa45000 psi
Tensile Strength, Yield 165 MPa
@Strain 0.5 %
23900 psi
@Strain 0.5 %
Elongation at Break 20 %20 %in 50 mm
Creep Strength  153 MPa
@Temperature 290 °C
22200 psi
@Temperature 554 °F
for 0.00001%/h
 224 MPa
@Temperature 230 °C
32500 psi
@Temperature 446 °F
for 0.00001%/h
Modulus of Elasticity 130 GPa18900 ksi
Compressive Strength 205 MPa29700 psiat permanent set of 1%
 395 MPa57300 psiat permanent set of 10%
Fatigue Strength 107 MPa
@# of Cycles 1.00e+8
15500 psi
@# of Cycles 1.00e+8
Reverse Bending
Machinability 70 %70 %UNS C36000 (free-cutting brass) = 100%
Charpy Impact 15.0 J11.1 ft-lbV-notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00003448 ohm-cm
@Temperature 20.0 °C
0.00003448 ohm-cm
@Temperature 68.0 °F
5% IACS, as-cast tempers
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 300 °C
9.44 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.375 J/g-°C0.0896 BTU/lb-°F
Thermal Conductivity 22.0 W/m-K
@Temperature 20.0 °C
153 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1108 - 1143 °C2026 - 2089 °F
Solidus 1108 °C2026 °F
Liquidus 1143 °C2089 °F
Shrinkage 1.1 %1.1 %Patternmaker's Shrinkage (1/8 in./ft.)
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 260 °C500 °FStress-Relieving Temperature; 1 h for each 25 mm of section thickness
Casting Temperature 1230 - 1320 °C2250 - 2410 °FHeavy castings
 1260 - 1430 °C2300 - 2610 °FLight castings
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0050 %<= 0.0050 %
Antimony, Sb <= 0.25 %<= 0.25 %
Copper, Cu 63 - 67 %63 - 67 %
Iron, Fe <= 1.5 %<= 1.5 %
Lead, Pb 3.0 - 5.0 %3.0 - 5.0 %
Manganese, Mn <= 1.0 %<= 1.0 %
Nickel, Ni 19 - 21.5 %19 - 21.5 %
Phosphorus, P <= 0.050 %<= 0.050 %
Silicon, Si <= 0.15 %<= 0.15 %
Sulfur, S <= 0.080 %<= 0.080 %
Tin, Sn 3.5 - 4.5 %3.5 - 4.5 %
Zinc, Zn 3.0 - 9.0 %3.0 - 9.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Leaded Nickel Bronze, UNS C97800, Copper Casting Alloy
Leaded Phosphor Bronze, UNS C94400, Copper Casting Alloy
Copper, UNS C62400 (Aluminum Bronze 11%)
High-Leaded Tin Bronze, UNS C93900, Copper Casting Alloy
Leaded High-Strength Yellow Brass, UNS C86700, Copper Casting Alloy

MC97600b1 / 11977

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.