Moplen EP440G is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP440G is a block copolymer typically used by customers in corrugated board and corrugated plastic applications for industrial packing. Moplen EP440G resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact. Product Features: Excellent processibility/High stiffness/High mechanical properties/High melt strength/High impact resistance at low temperature Typical Applications: Corrugated board/Rigid sheet/Corrugated plastic for industrial packing and for advertising box Information provided by PolyMirae |